In normal sintering of iron ore, there is a wide difference in temperature of the sinter bed between top and bottom; i.e. the flame front temperature of the sinter bed gradually increases towards the bottom because the lower part gets longer time for drying and preheating by exit gas. Therefore, the top part may have insufficient fusion and the bottom is excessively fused. Thus, sinter quality may become inhomogeneous and the coke breeze requirement becomes higher than the actual thermal requirement. If it is charged in multiple layers; e.g. higher amount of coke at the top and a lower amount of coke at the bottom, heat will be homogeneously distributed and the actual coke requirement would be lower than the existing. However, no study has ...
Recently, coke in an iron ore sintering process is replaced in part by powdered anthracite; less exp...
This paper presents a number of factors influencing Sinter Quality like particle grain size which re...
This investigation deals with the effect of replacing some amount of Baharia high barite iron ore co...
In iron ore sintering, effective segregation of the particulate bed on the strand can result in prod...
This study investigates the sintering behavior of iron ore and its modification regarding the conven...
In an iron ore sintering bed, the combustion behaviour of coke particles together with velocity of t...
The present investigation deals with the sinterability of Goa (India) iron ore having high Fe (65.2%...
Carbon combustion rates can be altered with different particle sizes of solid fuel, which can direct...
The present investigation deals with the sinterability of Goa (India) iron ore having high Fe (65...
An investigation was carried out into the use of saw-dust form oak wood as a supplementary fuel in t...
The objective of the present investigation was to under-stand the problems associated with the pr...
The contemporary shaft furnaces for the production of magnesia sinter have a very good performance i...
The testing cycle, described in the paper, included fine-grained coke breeze granulation tests and i...
The fuel segregation distribution sintering process, with a high fuel dosage in upper layer and a lo...
In a conventional sintering process, heat deficiency at the top layer of sinter-bed causes poor qual...
Recently, coke in an iron ore sintering process is replaced in part by powdered anthracite; less exp...
This paper presents a number of factors influencing Sinter Quality like particle grain size which re...
This investigation deals with the effect of replacing some amount of Baharia high barite iron ore co...
In iron ore sintering, effective segregation of the particulate bed on the strand can result in prod...
This study investigates the sintering behavior of iron ore and its modification regarding the conven...
In an iron ore sintering bed, the combustion behaviour of coke particles together with velocity of t...
The present investigation deals with the sinterability of Goa (India) iron ore having high Fe (65.2%...
Carbon combustion rates can be altered with different particle sizes of solid fuel, which can direct...
The present investigation deals with the sinterability of Goa (India) iron ore having high Fe (65...
An investigation was carried out into the use of saw-dust form oak wood as a supplementary fuel in t...
The objective of the present investigation was to under-stand the problems associated with the pr...
The contemporary shaft furnaces for the production of magnesia sinter have a very good performance i...
The testing cycle, described in the paper, included fine-grained coke breeze granulation tests and i...
The fuel segregation distribution sintering process, with a high fuel dosage in upper layer and a lo...
In a conventional sintering process, heat deficiency at the top layer of sinter-bed causes poor qual...
Recently, coke in an iron ore sintering process is replaced in part by powdered anthracite; less exp...
This paper presents a number of factors influencing Sinter Quality like particle grain size which re...
This investigation deals with the effect of replacing some amount of Baharia high barite iron ore co...