This dataset contains the raw data of figure 1-8 in the journal paper: Fermi level tuning of ZnO films through supercycled atomic layer deposition which has been accepted by Nanoscale Research Letter (Springer) on 08/09/2017.</span
ZnO is a remarkable material with many applications in electronics and catalysis. Atomic layer depos...
Atmospheric pressure spatial atomic layer deposition (AP-SALD) has recently emerged as an appealing ...
This is a dataset of the all of the raw data used to produce the journal article titled "Hierarchica...
Process details for one growth supercycle in the supercycled ALD process used in this study. Figure ...
A novel supercycled atomic layer deposition (ALD) process which combines thermal ALD process with in...
This dataset contains all of the original data used in the preparation of the publication titled "Hi...
Abstract A novel supercycled atomic layer deposition (ALD) process which combines thermal ALD proces...
This dataset contains the raw data of figure 1-7 in the journal paper: Huang, R. (2017). Compliance...
This is the open dataset for the paper: "Demelius, L. et al. Shedding light on the initial growth of...
An innovative approach towards the physico-chemical tailoring of zinc oxide thin films is reported. ...
This data article is related to our recently published article (Hussain et al., in press [1]) where ...
<p>Briefing of the structural and optical properties of synthesized ZnO nanosheets at different calc...
AbstractThis data article is related to our recently published article (Hussain et al., in press [1]...
Supplementary experimental data for ZnO films grown on MgO (111). Table S1. Detailed growth conditio...
The files for computing the Figures are in the surface and subsurface files. All the figures can be ...
ZnO is a remarkable material with many applications in electronics and catalysis. Atomic layer depos...
Atmospheric pressure spatial atomic layer deposition (AP-SALD) has recently emerged as an appealing ...
This is a dataset of the all of the raw data used to produce the journal article titled "Hierarchica...
Process details for one growth supercycle in the supercycled ALD process used in this study. Figure ...
A novel supercycled atomic layer deposition (ALD) process which combines thermal ALD process with in...
This dataset contains all of the original data used in the preparation of the publication titled "Hi...
Abstract A novel supercycled atomic layer deposition (ALD) process which combines thermal ALD proces...
This dataset contains the raw data of figure 1-7 in the journal paper: Huang, R. (2017). Compliance...
This is the open dataset for the paper: "Demelius, L. et al. Shedding light on the initial growth of...
An innovative approach towards the physico-chemical tailoring of zinc oxide thin films is reported. ...
This data article is related to our recently published article (Hussain et al., in press [1]) where ...
<p>Briefing of the structural and optical properties of synthesized ZnO nanosheets at different calc...
AbstractThis data article is related to our recently published article (Hussain et al., in press [1]...
Supplementary experimental data for ZnO films grown on MgO (111). Table S1. Detailed growth conditio...
The files for computing the Figures are in the surface and subsurface files. All the figures can be ...
ZnO is a remarkable material with many applications in electronics and catalysis. Atomic layer depos...
Atmospheric pressure spatial atomic layer deposition (AP-SALD) has recently emerged as an appealing ...
This is a dataset of the all of the raw data used to produce the journal article titled "Hierarchica...