Some of the foundries are in need of meeting production targets and due to the urgency they ignore the rejections. The objective of this paper is to analyze the various defects, [1] from molding process in a cast iron foundry. The Failure Mode Effects Analysis (FMEA) in quality control [2-6] with suitable supply chain for mold making process considering rejection rates are identified and analyzed in terms of Risk Priority Number (RPN) to prioritize the attention for each of the problem. The optimum levels of selected parameters [7] are obtained in this analysis
This paper aims to present a modified failure mode and effects analysis (FMEA) in order to make the ...
The FMEA (Failure Mode and Effects Analysis) method consists in analysis of failure modes and evalua...
Casting process is the most widely used process in manufacturing industries especially in automotive...
Some of the foundries are in need of meeting production targets and due to the urgency they ignore t...
This paper proposes a novel strategy to finalize the mould design of a specific cast component throu...
Determining the cause of the dominant suitability in a process is the final goal of this study, so t...
The present paper studies the reliability analysis of the casting process in foundry work using a pr...
The aim of the paper is to highlight the significance of implication of risk analysis and quality co...
Abstract--- The study has attempted to present an effective tool for solving the problem of manufact...
Production of casting involves various processes like pattern making, moulding, core making and melt...
The problem that occurs in the production of sintered ore is the number of defective products. In th...
The paper presents issues of quality management related to iron casts manufactured on automated foun...
The present paper explores advanced approaches to the FMEA method (Failure Mode and Effect Analysis)...
Along with the advancement of the industrial world, the competition between companies is getting tou...
In service and production area, problems such as severity of competition and increasing customers’ e...
This paper aims to present a modified failure mode and effects analysis (FMEA) in order to make the ...
The FMEA (Failure Mode and Effects Analysis) method consists in analysis of failure modes and evalua...
Casting process is the most widely used process in manufacturing industries especially in automotive...
Some of the foundries are in need of meeting production targets and due to the urgency they ignore t...
This paper proposes a novel strategy to finalize the mould design of a specific cast component throu...
Determining the cause of the dominant suitability in a process is the final goal of this study, so t...
The present paper studies the reliability analysis of the casting process in foundry work using a pr...
The aim of the paper is to highlight the significance of implication of risk analysis and quality co...
Abstract--- The study has attempted to present an effective tool for solving the problem of manufact...
Production of casting involves various processes like pattern making, moulding, core making and melt...
The problem that occurs in the production of sintered ore is the number of defective products. In th...
The paper presents issues of quality management related to iron casts manufactured on automated foun...
The present paper explores advanced approaches to the FMEA method (Failure Mode and Effect Analysis)...
Along with the advancement of the industrial world, the competition between companies is getting tou...
In service and production area, problems such as severity of competition and increasing customers’ e...
This paper aims to present a modified failure mode and effects analysis (FMEA) in order to make the ...
The FMEA (Failure Mode and Effects Analysis) method consists in analysis of failure modes and evalua...
Casting process is the most widely used process in manufacturing industries especially in automotive...