Using NASA IIb as a base composition, the effects of five key elements (carbon, tungsten, tantalum, aluminum, and hafnium) on resultant properties were investigated in an effort to optimize the composition and derive new wrought high temperature alloys with improved strength characteristics. A total of nineteen compositions were melted, extruded, and rolled to bar stock using thermomechanical processing. Both full and partial solution heat treatments were developed for the compositions. Tensile properties from room temperature to 1800 deg F, stress and creep rupture properties to 1800 deg F, and thermal stability characteristics were evaluated. NASA IIb-7 exhibited the best response to the partial solution heat treatment for optimum propert...
Superalloys show a good combination of mechanical strength and resistance to surface degradation und...
Alloy product is high strength, high temperature nickel base material with higher incipient melting ...
Nickel-manganese electroformed specimens and nickel-cobalt-manganese samples were heat treated at 34...
A program was conducted to optimize the composition of NASA IIb-11, an alloy originally developed as...
Alloy has high temperature properties exceeding strength of all known superalloys. It exhibits inher...
An investigation was conducted to provide an advanced-temperature nickel-base alloy with properties ...
Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the str...
Bar stock of the NASA-TRW 6-A alloy was made by prealloyed powder techniques and its properties eval...
Melting and casting procedures, strength and ductility, oxidation resistance, and metallurgy of new ...
Argon atomized nickel alloys processed thermochemically for use at high temperature
The data obtained during this and previous programs indicate that the VM-103 has useful strength at ...
Two dispersion strengthened nickel base alloy systems were developed for use at temperatures up to 1...
A nickel-base superalloy based on the nickel-aluminum-tungsten system designated WAZ-16 was develope...
Strength and workability of high temperature nickel-base, cobalt-base, and cobalt-refractory metal s...
Superalloys show a good combination of mechanical strength and resistance to surface degradation und...
Superalloys show a good combination of mechanical strength and resistance to surface degradation und...
Alloy product is high strength, high temperature nickel base material with higher incipient melting ...
Nickel-manganese electroformed specimens and nickel-cobalt-manganese samples were heat treated at 34...
A program was conducted to optimize the composition of NASA IIb-11, an alloy originally developed as...
Alloy has high temperature properties exceeding strength of all known superalloys. It exhibits inher...
An investigation was conducted to provide an advanced-temperature nickel-base alloy with properties ...
Nickel-base superalloy has a strength of 20,000 psi at 2,200 degrees F, approximately double the str...
Bar stock of the NASA-TRW 6-A alloy was made by prealloyed powder techniques and its properties eval...
Melting and casting procedures, strength and ductility, oxidation resistance, and metallurgy of new ...
Argon atomized nickel alloys processed thermochemically for use at high temperature
The data obtained during this and previous programs indicate that the VM-103 has useful strength at ...
Two dispersion strengthened nickel base alloy systems were developed for use at temperatures up to 1...
A nickel-base superalloy based on the nickel-aluminum-tungsten system designated WAZ-16 was develope...
Strength and workability of high temperature nickel-base, cobalt-base, and cobalt-refractory metal s...
Superalloys show a good combination of mechanical strength and resistance to surface degradation und...
Superalloys show a good combination of mechanical strength and resistance to surface degradation und...
Alloy product is high strength, high temperature nickel base material with higher incipient melting ...
Nickel-manganese electroformed specimens and nickel-cobalt-manganese samples were heat treated at 34...