AbstractNanoindentation is a useful method to probe the material properties of a solid. Its effective use lies in interpreting the data collected from a nanoindentation experiment with an associated analytical/numerical solution of the corresponding problem configuration. In this paper, a parametric finite element study has been performed to develop a new procedure for extracting elastic–plastic properties of a material through nanoindentation experiments with a substantially improved accuracy for the elastic properties of a elastic–plastic solid. The procedure involves data collected through the use of two, different, nanoindenter tips. Non-dimensional functions were constructed for two different indenter geometries to show that test resul...
Thesis (Ph.D.)--Wichita State University, College of Engineering, Dept. of Industrial and Manufactur...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
AbstractMaterial properties such as hardness can be dependent on the size of the indentation load wh...
AbstractNanoindentation is a useful method to probe the material properties of a solid. Its effectiv...
Nanoindentation is a widely used state of the art facility to precisely and conveniently evaluate th...
AbstractThe conventional method to extract elastic properties in the nanoindentation of linearly ela...
This study examines the accuracy of the extracted elastic properties using nanoindentation. Since th...
The nanoindentation test is frequently used as an alternate method to obtain the mechanical properti...
This is the first of two papers associated with materials characterization methods based on hardness...
AbstractNanoindentation is a powerful technique used for assessing mechanical properties at nano/mic...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
Journal Of Materials Research, 21(10), 2628-2637. http://dx.doi.org/10.1557/JMR.2006.0324Instrumente...
Instrumented nanoindentation tests have reached an effective level of theoretical and practical kno...
The nanoindentation test is frequently used as an alternate method to obtain the mechanical properti...
Thesis (Ph.D.)--Wichita State University, College of Engineering, Dept. of Industrial and Manufactur...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
AbstractMaterial properties such as hardness can be dependent on the size of the indentation load wh...
AbstractNanoindentation is a useful method to probe the material properties of a solid. Its effectiv...
Nanoindentation is a widely used state of the art facility to precisely and conveniently evaluate th...
AbstractThe conventional method to extract elastic properties in the nanoindentation of linearly ela...
This study examines the accuracy of the extracted elastic properties using nanoindentation. Since th...
The nanoindentation test is frequently used as an alternate method to obtain the mechanical properti...
This is the first of two papers associated with materials characterization methods based on hardness...
AbstractNanoindentation is a powerful technique used for assessing mechanical properties at nano/mic...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
Journal Of Materials Research, 21(10), 2628-2637. http://dx.doi.org/10.1557/JMR.2006.0324Instrumente...
Instrumented nanoindentation tests have reached an effective level of theoretical and practical kno...
The nanoindentation test is frequently used as an alternate method to obtain the mechanical properti...
Thesis (Ph.D.)--Wichita State University, College of Engineering, Dept. of Industrial and Manufactur...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
AbstractMaterial properties such as hardness can be dependent on the size of the indentation load wh...