AbstractThe conventional method to extract elastic properties in the nanoindentation of linearly elastic solids relies primarily on Sneddon’s solution (1948). The underlying assumptions behind Sneddon’s derivation, namely, (1) an infinitely large incompressible specimen; (2) an infinitely sharp indenter tip, are generally violated in nanoindentation. As such, correction factors are commonly introduced to achieve accurate measurements. However, little is known regarding the relationship between the correction factors and how they affect the overall accuracy. This paper first proposes a criterion for the specimen’s geometry to comply with the first assumption, and modifies Sneddon’s elastic relation to account for the finite tip radius effect...
The nanoindentation technique has made it possible to measure deformations at extremely low forces a...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
This is the first of two papers associated with materials characterization methods based on hardness...
AbstractThe conventional method to extract elastic properties in the nanoindentation of linearly ela...
This study examines the accuracy of the extracted elastic properties using nanoindentation. Since th...
AbstractNanoindentation is a useful method to probe the material properties of a solid. Its effectiv...
2006-2007 > Academic research: refereed > Publication in refereed journalVersion of RecordPublishe
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
AbstractNanoindentation is a powerful technique used for assessing mechanical properties at nano/mic...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
International audienceIn the Sneddon relationship between unloading contact stiffness, elastic modul...
Methods currently used for analyzing nanoindentation load-displacement data to determine a material`...
Thesis (Ph.D.)--Wichita State University, College of Engineering, Dept. of Industrial and Manufactur...
Nanoindentation is a widely used state of the art facility to precisely and conveniently evaluate th...
Journal Of Materials Research, 21(10), 2628-2637. http://dx.doi.org/10.1557/JMR.2006.0324Instrumente...
The nanoindentation technique has made it possible to measure deformations at extremely low forces a...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
This is the first of two papers associated with materials characterization methods based on hardness...
AbstractThe conventional method to extract elastic properties in the nanoindentation of linearly ela...
This study examines the accuracy of the extracted elastic properties using nanoindentation. Since th...
AbstractNanoindentation is a useful method to probe the material properties of a solid. Its effectiv...
2006-2007 > Academic research: refereed > Publication in refereed journalVersion of RecordPublishe
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
AbstractNanoindentation is a powerful technique used for assessing mechanical properties at nano/mic...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
International audienceIn the Sneddon relationship between unloading contact stiffness, elastic modul...
Methods currently used for analyzing nanoindentation load-displacement data to determine a material`...
Thesis (Ph.D.)--Wichita State University, College of Engineering, Dept. of Industrial and Manufactur...
Nanoindentation is a widely used state of the art facility to precisely and conveniently evaluate th...
Journal Of Materials Research, 21(10), 2628-2637. http://dx.doi.org/10.1557/JMR.2006.0324Instrumente...
The nanoindentation technique has made it possible to measure deformations at extremely low forces a...
Nowadays many indentation techniques are being commonly employed for determining some mechanical pro...
This is the first of two papers associated with materials characterization methods based on hardness...