The paper documents metallurgical possibilities of high alloy cast steel production in open induction medium frequency furnaces and an electric arc furnace in a gravity die casting foundry. The observation was focused on the emergence of gas defects in steel castings. The content of gases achieved during the metallurgical processes was evaluated for every unit of the production equipment and the casting ladle before casting into disposable sand moulds. The sand mould area was considered to be constant. The aim was to evaluate the current metallurgical possibilities of affecting the content of gases in high alloy cast steel in the current technical conditions of the foundry
Abstract The mechanical properties of steel components are controlled by the chemical composition an...
This paper is presented with the intention to examine some of the steel production problems in Ind...
The changes of a sulphur content during refining in melting low-alloy and high-alloy steels (G17CrMo...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper presents an analysis, regarding the control of the possible dangerous leaks of carbon mono...
A content of this thesis is an analysis of a steel castings production mismatch in Tatra Metallurgy ...
Obsahem diplomové práce je rozbor vad a neshodné výroby ocelových odlitků ve slévárně Tatra Metalurg...
Przedstawione w artykule zagadnienia dotykają problemu wad gazowych występujących w Odlewni Żeliwa. ...
Use of welding technology for the repair of steel castings is particularly common in two areas. Thes...
The need to develop products with special characteristics and high mechanical properties led to the ...
This paper is presented with the intention to examine some of the steel production problems in Ind...
The article is focused on the use of the measurement of oxygen activity for the management of cast-i...
Součástí diplomové práce je část teoretická a část praktická. V teoretické části se zaměřuji na vliv...
Abstract The mechanical properties of steel components are controlled by the chemical composition an...
This paper is presented with the intention to examine some of the steel production problems in Ind...
The changes of a sulphur content during refining in melting low-alloy and high-alloy steels (G17CrMo...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper documents metallurgical possibilities of high alloy cast steel production in open inductio...
The paper presents an analysis, regarding the control of the possible dangerous leaks of carbon mono...
A content of this thesis is an analysis of a steel castings production mismatch in Tatra Metallurgy ...
Obsahem diplomové práce je rozbor vad a neshodné výroby ocelových odlitků ve slévárně Tatra Metalurg...
Przedstawione w artykule zagadnienia dotykają problemu wad gazowych występujących w Odlewni Żeliwa. ...
Use of welding technology for the repair of steel castings is particularly common in two areas. Thes...
The need to develop products with special characteristics and high mechanical properties led to the ...
This paper is presented with the intention to examine some of the steel production problems in Ind...
The article is focused on the use of the measurement of oxygen activity for the management of cast-i...
Součástí diplomové práce je část teoretická a část praktická. V teoretické části se zaměřuji na vliv...
Abstract The mechanical properties of steel components are controlled by the chemical composition an...
This paper is presented with the intention to examine some of the steel production problems in Ind...
The changes of a sulphur content during refining in melting low-alloy and high-alloy steels (G17CrMo...