Emphasis has been placed on determining the interrelations among the composition, phase structure, deformation, and fracture properties of the alpha phase in susceptible alpha-beta alloys. The program is divided into two parts: (1) evaluation of the aqueous stress corrosion susceptibility of a series of alloys that contain various alpha-soluble elements; and (2) investigations of the metallurgical aspects of the mechanism of aqueous stress corrosion cracking
Titanium alloy stress corrosion cracking at ambient temperature in aqueous salt solution
Two principle areas studied were stress corrosion crack growth rates of a titanium alloy in liquid e...
Susceptibility of titanium alloys to hot-salt stress-corrosion cracking increased as follows: Ti-2Al...
A detailed study was made of the relation between the size distribution of Ti3Al particles in a Ti-8...
Metal composition effects on stress corrosion cracking of titanium alloys in nitrogen tetroxide, wat...
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
Stress corrosion cracking tests of titanium alloys at ambient temperature in aqueous solution
Stress corrosion tests of titanium alloys in distilled and aqueous salt solutions at ambient tempera...
Aluminum concentration effects on stress corrosion cracking of titanium alloys in aqueous solution
Stress corrosion cracking susceptibility of titanium alloys in nitrogen tetroxide and aqueous and ho...
Stress corrosion data for titanium alloys in aqueous, hot salt, and nitrogen dioxide environment
Aluminum concentration effects on stress corrosion cracking of titanium alloys at ambient temperatur...
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
This report investigates stress corrosion cracking susceptibility of titanium alloys in nitrogen tet...
Titanium alloy stress corrosion cracking at ambient temperature in aqueous salt solution
Two principle areas studied were stress corrosion crack growth rates of a titanium alloy in liquid e...
Susceptibility of titanium alloys to hot-salt stress-corrosion cracking increased as follows: Ti-2Al...
A detailed study was made of the relation between the size distribution of Ti3Al particles in a Ti-8...
Metal composition effects on stress corrosion cracking of titanium alloys in nitrogen tetroxide, wat...
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
Stress corrosion cracking tests of titanium alloys at ambient temperature in aqueous solution
Stress corrosion tests of titanium alloys in distilled and aqueous salt solutions at ambient tempera...
Aluminum concentration effects on stress corrosion cracking of titanium alloys in aqueous solution
Stress corrosion cracking susceptibility of titanium alloys in nitrogen tetroxide and aqueous and ho...
Stress corrosion data for titanium alloys in aqueous, hot salt, and nitrogen dioxide environment
Aluminum concentration effects on stress corrosion cracking of titanium alloys at ambient temperatur...
Stress corrosion cracking of titanium alloys at ambient temperature in aqueous solution
This report investigates stress corrosion cracking susceptibility of titanium alloys in nitrogen tet...
Titanium alloy stress corrosion cracking at ambient temperature in aqueous salt solution
Two principle areas studied were stress corrosion crack growth rates of a titanium alloy in liquid e...
Susceptibility of titanium alloys to hot-salt stress-corrosion cracking increased as follows: Ti-2Al...