This paper explores the feasibility of characterizing the mechanical response of the commercial aerospace grade epoxy resin RTM6 by nanoindentation tests at varying temperatures and strain rates. Since glassy polymers exhibit time-dependent mechanical properties, a dynamic nanoindentation technique was used. This method consists on superimposing a small sinusoidal force oscillation on the applied force. Viscoelastic properties are then characterized by their storage and loss moduli, whereas the visco-plastic response of the material can be associated to its hardness. In such experiments, thermal stability of the measuring technique is critical to achieve a low thermal drift and it becomes increasingly important as the measuring temperature ...
This is a report of the inter-relationships between mechanical properties of glassy polymers, obtain...
Quasi-static nanoindentation has been used to assess the mechanical properties of soft and spatially...
The purpose of this work was to explore the possibility of measuring properties of viscoelastic mate...
Nanoindentation has a high load resolution, depth sensing capabilities, and can be used to character...
The effect of loading force, loading rate and unloading rate on the viscoelastic behavior of three r...
During sharp contacts, polymeric materials can exhibit elastic (reversible), plastic (instantaneous ...
Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight polymer m...
ABSTRACT—Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight ...
The aim of this PhD work is to develop a novel and effective instrument to characterize the mechanic...
The high degree of heterogeneity of polymeric materials makes it difficult to describe their overall...
Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight polymer m...
The Atomic Force Microscope (AFM), apart form its conventional use as a microscope, is also used for...
The Atomic Force Microscope (AFM), apart form its conventional use as a microscope, is also used for...
ABSTRACT: Motivated by recent progress in viscoelastic indentation analysis, the identification of v...
The purpose of this work is to further develop experimental methodologies using flat punch nanoinden...
This is a report of the inter-relationships between mechanical properties of glassy polymers, obtain...
Quasi-static nanoindentation has been used to assess the mechanical properties of soft and spatially...
The purpose of this work was to explore the possibility of measuring properties of viscoelastic mate...
Nanoindentation has a high load resolution, depth sensing capabilities, and can be used to character...
The effect of loading force, loading rate and unloading rate on the viscoelastic behavior of three r...
During sharp contacts, polymeric materials can exhibit elastic (reversible), plastic (instantaneous ...
Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight polymer m...
ABSTRACT—Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight ...
The aim of this PhD work is to develop a novel and effective instrument to characterize the mechanic...
The high degree of heterogeneity of polymeric materials makes it difficult to describe their overall...
Nanoindentation testing was used to determine the dynamic viscoelastic properties of eight polymer m...
The Atomic Force Microscope (AFM), apart form its conventional use as a microscope, is also used for...
The Atomic Force Microscope (AFM), apart form its conventional use as a microscope, is also used for...
ABSTRACT: Motivated by recent progress in viscoelastic indentation analysis, the identification of v...
The purpose of this work is to further develop experimental methodologies using flat punch nanoinden...
This is a report of the inter-relationships between mechanical properties of glassy polymers, obtain...
Quasi-static nanoindentation has been used to assess the mechanical properties of soft and spatially...
The purpose of this work was to explore the possibility of measuring properties of viscoelastic mate...