19. KEY WORDS (Continue on reverie aide It neceeary and Identity by block number) Melt-spinning, splat-quenching, crystallisation, eutectic. superplasticity 20. ABSTRACT (Continue on reveree side It neceeeary and Identify by block number) This paper described the microstructure and mechanical properties of Pb-Sn eutectic alloys prepared by melt-spinnin
AbstractA eutectic lead–tin alloy was prepared by melting the commercially pure metals and cast in c...
The reason for the superior flowability of a melt in the neighborhood of the eutectic composition in...
Results of a study on microstructural evolution of eutectic Sn-57wt.% Bi processed with cooling rate...
Experiments were conducted on a Pb-62% Sn eutectic alloy containing 160 ppm of Sb. The alloy was pro...
Melt undercooling opens new solidification pathways for non-equilibrium phases and non-conventional ...
Thin metallic films of Pb/Sn eutectic alloy prepared by a melting method were examined. Direct study...
The Pb-Sn alloy has a wide use in the electronic, energy storage and nuclear industries and a fine-g...
The Pb-Sn alloy has a wide use in the electronic, energy storage and nuclear industries and a fine-...
The Pb–62% Sn eutectic alloy was processed by equal-channel angular pressing and then tested in tens...
The Sn-Co-Cu eutectic solder alloy is a less expensive and is therefore a possible alternative to th...
Two eutectic alloys Bi-Ag and Bi-Zn were rapidly solidified using melt-spinning technique. X-ray dif...
Results of a study on microstructural evolution of eutectic Sn-57 wt.% Bi processed with cooling rat...
The structure of liquid Sn0.739Pb0.261 and Sn0.57Bi0.43 eutectic alloys was studied by means of X-ra...
The physical properties (viscosity, density, electroresistivity and magnetic susceptibility) of pure...
The physical properties (viscosity, density, electroresistivity and magnetic susceptibility) of pure...
AbstractA eutectic lead–tin alloy was prepared by melting the commercially pure metals and cast in c...
The reason for the superior flowability of a melt in the neighborhood of the eutectic composition in...
Results of a study on microstructural evolution of eutectic Sn-57wt.% Bi processed with cooling rate...
Experiments were conducted on a Pb-62% Sn eutectic alloy containing 160 ppm of Sb. The alloy was pro...
Melt undercooling opens new solidification pathways for non-equilibrium phases and non-conventional ...
Thin metallic films of Pb/Sn eutectic alloy prepared by a melting method were examined. Direct study...
The Pb-Sn alloy has a wide use in the electronic, energy storage and nuclear industries and a fine-g...
The Pb-Sn alloy has a wide use in the electronic, energy storage and nuclear industries and a fine-...
The Pb–62% Sn eutectic alloy was processed by equal-channel angular pressing and then tested in tens...
The Sn-Co-Cu eutectic solder alloy is a less expensive and is therefore a possible alternative to th...
Two eutectic alloys Bi-Ag and Bi-Zn were rapidly solidified using melt-spinning technique. X-ray dif...
Results of a study on microstructural evolution of eutectic Sn-57 wt.% Bi processed with cooling rat...
The structure of liquid Sn0.739Pb0.261 and Sn0.57Bi0.43 eutectic alloys was studied by means of X-ra...
The physical properties (viscosity, density, electroresistivity and magnetic susceptibility) of pure...
The physical properties (viscosity, density, electroresistivity and magnetic susceptibility) of pure...
AbstractA eutectic lead–tin alloy was prepared by melting the commercially pure metals and cast in c...
The reason for the superior flowability of a melt in the neighborhood of the eutectic composition in...
Results of a study on microstructural evolution of eutectic Sn-57wt.% Bi processed with cooling rate...