We estimate effective radii of a spherical nanoindenter at various indentation depths using Hertz elastic contact theory for the fully elastic contact region and AFM profiling residual indentation marks for the elastoplastic contact region. Using frame compliance measured as a function of indentation depth and the concept of infinitesimal deformation of a spherical nanoindenter, we introduce a profile of indentation-depth-dependent frame compliance that successfully explains the variation in frame compliance over the entire contact region. After using this indentation-depth-dependent frame compliance, we evaluated more consistent indenter radii from Hertz elastic contact theory at shallow indentation depths (<90 nm).close1
Using dimensional analysis and finite element calculation, we studied spherical indentation in elast...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
Simulating complex interactions at different length scales of a hierarchical material system is esse...
The nanoindentation technique has made it possible to measure deformations at extremely low forces a...
We introduce a novel method to correct for imperfect indenter geometry and frame compliance in instr...
Nanoindentation with spherical tipped indenters provides a powerful technique for exploring surface ...
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
If all components in a nanoindentation system are well calibrated and a reference material has uniqu...
International audienceKnowledge of the relationship between the penetration depth and the contact ra...
International audienceInstrumented indentation experiments, where load and depth of penetration are ...
International audienceIn the Sneddon relationship between unloading contact stiffness, elastic modul...
An overview of development of indentation techniques and connections between contact mechanics and m...
International audienceAn experimental method to determine contact radius changes during a spherical ...
International audienceA correction factor for applying previous method proposed by Collin et al. (20...
International audienceThe study of analytical models for the determination of the contact radius bet...
Using dimensional analysis and finite element calculation, we studied spherical indentation in elast...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
Simulating complex interactions at different length scales of a hierarchical material system is esse...
The nanoindentation technique has made it possible to measure deformations at extremely low forces a...
We introduce a novel method to correct for imperfect indenter geometry and frame compliance in instr...
Nanoindentation with spherical tipped indenters provides a powerful technique for exploring surface ...
Nanoindentation techniques provide a unique opportunity to obtain mechanical properties of materials...
If all components in a nanoindentation system are well calibrated and a reference material has uniqu...
International audienceKnowledge of the relationship between the penetration depth and the contact ra...
International audienceInstrumented indentation experiments, where load and depth of penetration are ...
International audienceIn the Sneddon relationship between unloading contact stiffness, elastic modul...
An overview of development of indentation techniques and connections between contact mechanics and m...
International audienceAn experimental method to determine contact radius changes during a spherical ...
International audienceA correction factor for applying previous method proposed by Collin et al. (20...
International audienceThe study of analytical models for the determination of the contact radius bet...
Using dimensional analysis and finite element calculation, we studied spherical indentation in elast...
Nanoindentation is a widely recognized method for characterizing the mechanical properties of thin f...
Simulating complex interactions at different length scales of a hierarchical material system is esse...