The γ’ strengthening phase in an advanced nickel-based superalloy, ATI 718Plus, was characterized using a blind source separation applied to a four dimensional X-ray microanalysis dataset obtained by scanning transmission electron microscopy. Selected patterns in the X-ray spectra identified by independent component analysis were found to be spatially and chemically representative of the matrix (γ) and precipitate phases (γ’) present in the superalloy, enabling their size, shape and distribution to be determined. The three dimensional chemical reconstruction of the microstructure may provide insight into the role of the various alloying elements in the evolution of the microstructure at the nano-scale.The research leading to these results h...
Les compositions des phases γ, γ' et DO22 dans le superalliage à base Nickel RSR 143 (76Ni-13A1-9Mo-...
The utilisation of next-generation superalloys is of utmost significance in the progression of conte...
It is continuously sought in superalloys to increase the mechanical strength at high working temper...
AbstractThe γ′ strengthening phase in an advanced nickel-based superalloy, ATI 718Plus, was characte...
Allvac 718Plus (718Plus) is a high strength, corrosion resistant nickel- based superalloy used for a...
ATI 718Plus® is a nickel-based superalloy developed to replace Inconel 718 in aero engines for stati...
The purpose of this project was to characterize the microstructural and microchemical effects of a p...
Phase separation of g0 precipitates determines the microstructure and mechanical properties of nick...
Tailoring the properties of intermetallic alloys and phases, which resemble the foundation of a vast...
Abstract- The combined techniques of atom probe field-ion microscopy and transmission electron micro...
Nickel-based single crystal superalloy blades have excellent high-temperature performance as the hot...
Abstract. Atom-probe field-ion microscopy (APFIM) is used to study partitioning of the alloying elem...
Superalloys are metallic alloys with specific microstructures and atoms in solid solution allowing g...
This article discusses challenges faced in the development of new Ni-based superalloys for applicati...
The knowledge of the chemical composition at the atomic level of alloys is essential to understand t...
Les compositions des phases γ, γ' et DO22 dans le superalliage à base Nickel RSR 143 (76Ni-13A1-9Mo-...
The utilisation of next-generation superalloys is of utmost significance in the progression of conte...
It is continuously sought in superalloys to increase the mechanical strength at high working temper...
AbstractThe γ′ strengthening phase in an advanced nickel-based superalloy, ATI 718Plus, was characte...
Allvac 718Plus (718Plus) is a high strength, corrosion resistant nickel- based superalloy used for a...
ATI 718Plus® is a nickel-based superalloy developed to replace Inconel 718 in aero engines for stati...
The purpose of this project was to characterize the microstructural and microchemical effects of a p...
Phase separation of g0 precipitates determines the microstructure and mechanical properties of nick...
Tailoring the properties of intermetallic alloys and phases, which resemble the foundation of a vast...
Abstract- The combined techniques of atom probe field-ion microscopy and transmission electron micro...
Nickel-based single crystal superalloy blades have excellent high-temperature performance as the hot...
Abstract. Atom-probe field-ion microscopy (APFIM) is used to study partitioning of the alloying elem...
Superalloys are metallic alloys with specific microstructures and atoms in solid solution allowing g...
This article discusses challenges faced in the development of new Ni-based superalloys for applicati...
The knowledge of the chemical composition at the atomic level of alloys is essential to understand t...
Les compositions des phases γ, γ' et DO22 dans le superalliage à base Nickel RSR 143 (76Ni-13A1-9Mo-...
The utilisation of next-generation superalloys is of utmost significance in the progression of conte...
It is continuously sought in superalloys to increase the mechanical strength at high working temper...