This dissertation presents the development of the novel mechanical testing technique of in situ nanoindentation in a transmission electron microscope (TEM). This technique makes it possible to simultaneously observe and quantify the mechanical behavior of nano-scale volumes of solids
Nanoindentation is a material testing method frequently used for studies of mechanical properties on...
Nanotechnologies have already attracted massive interest in multiple fields of science and industry....
International audienceFundamental understanding and quantitative characterization of electron transp...
This dissertation presents the development of the novel mechanical testing technique of in situ nan...
International audienceThis chapter focuses on the nanoindentation of nanoparticles. It presents the ...
In-situ transmission electron microscopy is an established experimental technique that permits direc...
This report describes the design, construction, and testing of a nanoindentation specimen holder use...
The technique of Nanoindentation in situ Transmission Electron Microscope has been implemented on a ...
Investigating and modeling the mechanical properties of materials is important for many applications...
This paper highlights future developments in the field of in-situ transmission electron microscopy,...
Small scale mechanical deformations have gained a significant interest over the past few decades, dr...
In nanoindentation, the occurrence of cracks, pileup, sink-in, or film delamination adds additional ...
cited By 22International audienceIn situ transmission electron microscopy (TEM) nanomechanical testi...
This paper highlights future developments in the field of in-situ transmission electron microscopy, ...
The great effort is being placed in the design of new characterization techniques and the constructi...
Nanoindentation is a material testing method frequently used for studies of mechanical properties on...
Nanotechnologies have already attracted massive interest in multiple fields of science and industry....
International audienceFundamental understanding and quantitative characterization of electron transp...
This dissertation presents the development of the novel mechanical testing technique of in situ nan...
International audienceThis chapter focuses on the nanoindentation of nanoparticles. It presents the ...
In-situ transmission electron microscopy is an established experimental technique that permits direc...
This report describes the design, construction, and testing of a nanoindentation specimen holder use...
The technique of Nanoindentation in situ Transmission Electron Microscope has been implemented on a ...
Investigating and modeling the mechanical properties of materials is important for many applications...
This paper highlights future developments in the field of in-situ transmission electron microscopy,...
Small scale mechanical deformations have gained a significant interest over the past few decades, dr...
In nanoindentation, the occurrence of cracks, pileup, sink-in, or film delamination adds additional ...
cited By 22International audienceIn situ transmission electron microscopy (TEM) nanomechanical testi...
This paper highlights future developments in the field of in-situ transmission electron microscopy, ...
The great effort is being placed in the design of new characterization techniques and the constructi...
Nanoindentation is a material testing method frequently used for studies of mechanical properties on...
Nanotechnologies have already attracted massive interest in multiple fields of science and industry....
International audienceFundamental understanding and quantitative characterization of electron transp...