Impression creep testing is a technique in which the deformation resulting from load applied via a rectangular indenter can be converted relatively straightforwardly into a proxy for creep minimum strain rate. This offers a valuable route to assess the creep performance ranking of in-service high temperature plant materials for a number of reasons: the small specimen size makes extraction feasible without significantly affecting the structural integrity of plant; the possibility to test a single specimen at several stresses or temperatures enables multiple assessments; and, increasingly, the maturity of underlying technical understanding and quality of results increases confidence in the technique. However, the method is not without challen...
Small specimen creep testing techniques are novel mechanical test techniques that have been develope...
The measured "minimum" creep rate in the impression creep (IC) test is currently obtained from a "st...
Destructive testing of creep exposed components is a powerful tool for evaluation of remaining lifet...
Impression creep testing is an established small-scale testing technique in which the indentation ra...
In-service monitoring of power plant components toward later stages of plant life requires several m...
The impression creep test is a small sample testing technique that has been used mostly for qualitat...
The process of standardisation of small specimen creep testing techniques, specifically the impressi...
The process of standardisation of small specimen creep testing techniques, specifically the impressi...
High temperature power plant components are now working far beyond their operative designed life. Th...
High temperature power plant components are now working far beyond their operative designed life. Es...
High temperature power plant components are now working far beyond their operative designed life. Es...
High temperature power plant components are now working far beyond their operative designed life. Es...
The small sample impression creep test method has recently been of interest, as it can give a good i...
Small specimen creep testing techniques are novel mechanical test techniques that have been develope...
The current Thesis describes for the first time based on extensive industrial data how small specime...
Small specimen creep testing techniques are novel mechanical test techniques that have been develope...
The measured "minimum" creep rate in the impression creep (IC) test is currently obtained from a "st...
Destructive testing of creep exposed components is a powerful tool for evaluation of remaining lifet...
Impression creep testing is an established small-scale testing technique in which the indentation ra...
In-service monitoring of power plant components toward later stages of plant life requires several m...
The impression creep test is a small sample testing technique that has been used mostly for qualitat...
The process of standardisation of small specimen creep testing techniques, specifically the impressi...
The process of standardisation of small specimen creep testing techniques, specifically the impressi...
High temperature power plant components are now working far beyond their operative designed life. Th...
High temperature power plant components are now working far beyond their operative designed life. Es...
High temperature power plant components are now working far beyond their operative designed life. Es...
High temperature power plant components are now working far beyond their operative designed life. Es...
The small sample impression creep test method has recently been of interest, as it can give a good i...
Small specimen creep testing techniques are novel mechanical test techniques that have been develope...
The current Thesis describes for the first time based on extensive industrial data how small specime...
Small specimen creep testing techniques are novel mechanical test techniques that have been develope...
The measured "minimum" creep rate in the impression creep (IC) test is currently obtained from a "st...
Destructive testing of creep exposed components is a powerful tool for evaluation of remaining lifet...