International audienceNanocomposite Sm2Co17–Cu particles have been fabricated by low energy comilling of mechanically alloyed Sm2Co17 particles with Cu nanoparticles. The x-ray diffraction analyses show that the diffraction crystallite size (DCS) of Sm2Co17 decreases with increasing comilling time. Scanning and transmission electron microscopy observation demonstrates that the particle size is in the range of the DCS and the Sm2Co17 particles are separated by Cu particles. The coercivity as well as the remanence ratio decreases with increasing milling time due to the grain size reduction and grain separation. The nanocomposite Sm2Co17–Cu exhibits suitable magnetic and microstructure properties for high-density recording
The microstructures and tensile properties of two ultrafine structured Cu–5vol%Al₂O₃ nanocomposite s...
In this paper, the phase compositions, microstructures, atomic structures, and magnetic properties o...
Single crystal SmCo5 nanoparticles with an average size of 3.5 nm are produced by cluster-beam depos...
International audienceSmCo3Cu2/alfa-Fe nanocomposites have been obtained by mechanical milling (MM) ...
Nanocrystalline composites of CuCoNi (x = 0, 10, 20 wt-%) alloys reinforced with 7.5 wt-% of interme...
Mechanically alloyed Sm–Co powders and Sm12 (Co,Cu,Ti) 88 powders are investigated. X-ray diffractio...
Nanocomposite structures composed of ferromagnetic particles dispersed in a matrix are systems in wh...
Sm2Co17-type high-temperature permanent magnets with composition Sm(Co, Fe, Cu, Ti)z are investigate...
In this study, nanocrystalline SmCo5 bulk magnets were prepared by hot-pressing of nanoflake powders...
Nanocomposite Sm2Co17-5wt% FeCo magnets were synthesized by high energy ball milling followed by con...
The effect of wheel speed as well as an additive Cr3C2 on the structure, crystalline texture, and ma...
The SmCo-based permanent magnets are drawing much more attention since the early 1970\u27s for their...
Isotropic Sm-Co nanoparticle powders with high coercivity were prepared by high-energy ball milling ...
Textured nanocrystalline SmCo5-Cu magnets are produced by high-pressure torsion (HPT) of powder blen...
Nanocomposite Sm(2)Co(17)-5 wt% FeCo magnets were synthesized by high energy ball milling followed b...
The microstructures and tensile properties of two ultrafine structured Cu–5vol%Al₂O₃ nanocomposite s...
In this paper, the phase compositions, microstructures, atomic structures, and magnetic properties o...
Single crystal SmCo5 nanoparticles with an average size of 3.5 nm are produced by cluster-beam depos...
International audienceSmCo3Cu2/alfa-Fe nanocomposites have been obtained by mechanical milling (MM) ...
Nanocrystalline composites of CuCoNi (x = 0, 10, 20 wt-%) alloys reinforced with 7.5 wt-% of interme...
Mechanically alloyed Sm–Co powders and Sm12 (Co,Cu,Ti) 88 powders are investigated. X-ray diffractio...
Nanocomposite structures composed of ferromagnetic particles dispersed in a matrix are systems in wh...
Sm2Co17-type high-temperature permanent magnets with composition Sm(Co, Fe, Cu, Ti)z are investigate...
In this study, nanocrystalline SmCo5 bulk magnets were prepared by hot-pressing of nanoflake powders...
Nanocomposite Sm2Co17-5wt% FeCo magnets were synthesized by high energy ball milling followed by con...
The effect of wheel speed as well as an additive Cr3C2 on the structure, crystalline texture, and ma...
The SmCo-based permanent magnets are drawing much more attention since the early 1970\u27s for their...
Isotropic Sm-Co nanoparticle powders with high coercivity were prepared by high-energy ball milling ...
Textured nanocrystalline SmCo5-Cu magnets are produced by high-pressure torsion (HPT) of powder blen...
Nanocomposite Sm(2)Co(17)-5 wt% FeCo magnets were synthesized by high energy ball milling followed b...
The microstructures and tensile properties of two ultrafine structured Cu–5vol%Al₂O₃ nanocomposite s...
In this paper, the phase compositions, microstructures, atomic structures, and magnetic properties o...
Single crystal SmCo5 nanoparticles with an average size of 3.5 nm are produced by cluster-beam depos...