We measured the magnetic losses and the complex permeability of amorphous and nanocrystalline ribbons from DC to 1 GHz by combined application of fluxmetric and transmission line methods. Two transverse field annealed Co-based amorphous alloys, ~13 µm and ~25 µm tick and two nanocrystalline Finemet type alloys, ~13 µm and ~20 µm tick, endowed with defined transverse magnetic anisotropy, were characterized
For the purpose of practical applications of the amorphous Fe_5Co_Si_B_ ribbon to high frequency mag...
International audienceSoft magnetic materials are at the core of electromagnetic devices. Planar tra...
Nanocrystalline soft magnetic materials are widely used in power electronic applications due to thei...
We highlight the challenges posed by the experimental and theoretical assessment of the magnetic los...
Finemet type alloys have been investigated from DC to 1 GHz at different induction levels upon diffe...
Permeability and coercivity are the most important parameters for the evaluation of soft magnetic ma...
Low-field initial permeability (μi) has been measured at several steps of nanocrystallization in fou...
The initial permeability μ_i, the loss factor tan δ, and the inverse quality factor tan δ/μ_i of Fe_...
The phenomenology of magnetization process and losses in amorphous and nanocrystalline ribbons and ...
The magnetization process in field annealed amorphous ribbons has been investigated from dc to 10 MH...
International audienceUltrasoft magnetic materials, such as amorphous, nanocrystalline, and polycrys...
The object of this work is the comparison of domain structure and off-diagonal magnetoimpedance effe...
The ferromagnetic resonance (FMR) in the frequency range of 0.5 to 12.5 GHz has been investigated as...
Broadband magnetic loss and damping behavior of Co-based amorphous ribbons and thin films have been ...
Complex permeability $(μ=μ_1-iμ_2)$ after-effect of near-zero magnetostrictive CoFeCrSiB amorphous a...
For the purpose of practical applications of the amorphous Fe_5Co_Si_B_ ribbon to high frequency mag...
International audienceSoft magnetic materials are at the core of electromagnetic devices. Planar tra...
Nanocrystalline soft magnetic materials are widely used in power electronic applications due to thei...
We highlight the challenges posed by the experimental and theoretical assessment of the magnetic los...
Finemet type alloys have been investigated from DC to 1 GHz at different induction levels upon diffe...
Permeability and coercivity are the most important parameters for the evaluation of soft magnetic ma...
Low-field initial permeability (μi) has been measured at several steps of nanocrystallization in fou...
The initial permeability μ_i, the loss factor tan δ, and the inverse quality factor tan δ/μ_i of Fe_...
The phenomenology of magnetization process and losses in amorphous and nanocrystalline ribbons and ...
The magnetization process in field annealed amorphous ribbons has been investigated from dc to 10 MH...
International audienceUltrasoft magnetic materials, such as amorphous, nanocrystalline, and polycrys...
The object of this work is the comparison of domain structure and off-diagonal magnetoimpedance effe...
The ferromagnetic resonance (FMR) in the frequency range of 0.5 to 12.5 GHz has been investigated as...
Broadband magnetic loss and damping behavior of Co-based amorphous ribbons and thin films have been ...
Complex permeability $(μ=μ_1-iμ_2)$ after-effect of near-zero magnetostrictive CoFeCrSiB amorphous a...
For the purpose of practical applications of the amorphous Fe_5Co_Si_B_ ribbon to high frequency mag...
International audienceSoft magnetic materials are at the core of electromagnetic devices. Planar tra...
Nanocrystalline soft magnetic materials are widely used in power electronic applications due to thei...