Interfacing ferromagnetic materials with topological insulators is an intriguing strategy in order to enhance spin-to-charge conversion mechanisms, paving the way toward highly efficient spin-based electronic devices. In particular, the use of large-scale deposition techniques is demanding for a sustainable and cost-effective industrial technology transfer. In this work, we study the magnetic properties of the Co/Sb2Te3 heterostructure, where the ferromagnetic Co layer is deposited by atomic layer deposition on top of the Sb2Te3 topological insulator, which is grown by metal organic chemical vapor deposition. In particular, broadband ferromagnetic resonance is employed to characterize the Co/Sb2Te3 system and the reference heterostructure C...
Thesis: S.M., Massachusetts Institute of Technology, Department of Electrical Engineering and Comput...
The combination of topological properties and magnetic order can lead to new quantum states and exot...
Magnetic topological insulators (TIs) are an ideal playground for the study of novel quantum phenome...
Interfacing ferromagnetic materials with topological insulators is an intriguing strategy in order t...
This dataset contains the raw data files connected with the figures included in the paper "Ferromagn...
Large-area antimony telluride (Sb2Te3) thin films are grown by a metal organic chemical vapor deposi...
Taking the full advantage of the conformal growth characterizing atomic layer deposition (ALD), the ...
Spin-charge interconversion phenomena at the interface between magnetic materials and topological in...
A [GeTe/Sb2Te3] superlattice is known as a topological insulator. It shows magnetic responses such a...
Most electronic devices are made of tiny transistors and capacitors. But there is a limitation on ho...
The area of spintronics has witnessed tremendous progress in the 21st century. During the 1980s and ...
Spin–orbit torque (SOT) magnetoresistive random-access memory (MRAM) devices have been proposed for ...
Interfacing topological insulators (TI) with ferromagnetic (FM) layers is a promising route towards ...
Using soft x-ray absorption spectroscopy we determined the chemical and magnetic properties of the m...
We present a comprehensive study of the crystal structure of the thin-film, ferromagnetic topologica...
Thesis: S.M., Massachusetts Institute of Technology, Department of Electrical Engineering and Comput...
The combination of topological properties and magnetic order can lead to new quantum states and exot...
Magnetic topological insulators (TIs) are an ideal playground for the study of novel quantum phenome...
Interfacing ferromagnetic materials with topological insulators is an intriguing strategy in order t...
This dataset contains the raw data files connected with the figures included in the paper "Ferromagn...
Large-area antimony telluride (Sb2Te3) thin films are grown by a metal organic chemical vapor deposi...
Taking the full advantage of the conformal growth characterizing atomic layer deposition (ALD), the ...
Spin-charge interconversion phenomena at the interface between magnetic materials and topological in...
A [GeTe/Sb2Te3] superlattice is known as a topological insulator. It shows magnetic responses such a...
Most electronic devices are made of tiny transistors and capacitors. But there is a limitation on ho...
The area of spintronics has witnessed tremendous progress in the 21st century. During the 1980s and ...
Spin–orbit torque (SOT) magnetoresistive random-access memory (MRAM) devices have been proposed for ...
Interfacing topological insulators (TI) with ferromagnetic (FM) layers is a promising route towards ...
Using soft x-ray absorption spectroscopy we determined the chemical and magnetic properties of the m...
We present a comprehensive study of the crystal structure of the thin-film, ferromagnetic topologica...
Thesis: S.M., Massachusetts Institute of Technology, Department of Electrical Engineering and Comput...
The combination of topological properties and magnetic order can lead to new quantum states and exot...
Magnetic topological insulators (TIs) are an ideal playground for the study of novel quantum phenome...