Niobium pentoxide was deposited using tBuN=Nb(NEt2)3 as niobium precursor by both thermal atomic layer deposition (ALD) and plasma-enhanced atomic layer deposition (PE-ALD) with H2O and O2 plasma as coreactants, respectively. The deposition temperature was varied between 150 and 350 °C in both ALD processes. Amorphous films were obtained in all cases. Self-limiting saturated growth was confirmed for both ALD processes along with high uniformity over a 200 mm Si wafer. The PE-ALD process enabled a higher growth per cycle (GPC) than the thermal ALD process (0.56 Å vs 0.38 Å at 200 °C, respectively), while the GPC decreases with increasing temperature in both cases. The high purity of the film was confirmed using Rutherford backscattering spec...