The hydrogen evolution and oxidation kinetics in NiMH batteries have been investigated under temperature-controlled, steady-state, overdischarging conditions within a temperature range of 10 and 50°C and at discharging currents of 1–330 mA (0.0009 to 0.3 C rate). In situ Raman spectroscopic analyses of the gas phase showed that hydrogen is the only gas evolving inside the battery during overdischarge at the above-mentioned conditions. The pressure increase could be very critical at low temperatures, leading to opening of the safety vent at relatively low discharging currents, for example, only 220 mA at 10°C. The polarization parameters for the hydrogen evolution reaction, such as Tafel slopes and exchange currents were determined at the di...