The oxidation behavior of nonoxide silicon-based ceramics was investigated. Various Si3N4 and SiC ceramics were examined after long term oxidation tests (.ltoreq.10,000 h) at 1500.degree. in ambient air. The oxidation of the materials obeyed a nearly parabolic mechanism. However, different characteristic oxidation processes at the surface and the microstructure were observed dependent on the chemical components of the ceramic materials. The diffusion of oxygen into the material and its further reaction in the bulk of the material were found to be the most critical factors during long term oxidation
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
Within this study, the oxidation behavior of SiHfBCN ceramic powders and monoliths was studied at te...
The present study is focussed on the oxidation behavior of nonoxide silicon-based ceramics. Various ...
In the present study nonoxide ceramic materials based on silicon nitride were evaluated with respect...
The oxidation behaviour of Y2O3 plus Al2O3-doped Si3N4 based ceramics was investigated in air up to ...
The oxidation behavior of polymer-derived amorphous SiAlCNs was studied in the temperature range of ...
The oxidation behavior of polymer-derived amorphous SiAlCNs was studied in the temperature range of ...
The oxidation behaviour of hot-pressed β-SiAlON ceramics with different densities has been investiga...
Sintered ceramics produced from two kinds of silicon nitride powder were oxidized at 1000 and 1400 d...
Structural ceramics are potential mold materials for hot embossing, due to their superior mechanical...
International audienceThe oxidation of a silicon nitride–titanium nitride ceramic has been studied. ...
The effect of oxidation on the room-temperature mechanical properties of silicon nitride ceramics wi...
International audienceThe rate of air oxidation towards 1,000degreesC of the Si3N4-bonded silicon ca...
Within this study, the oxidation behavior of SiHfBCN ceramic powders and monoliths was studied at te...
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
Within this study, the oxidation behavior of SiHfBCN ceramic powders and monoliths was studied at te...
The present study is focussed on the oxidation behavior of nonoxide silicon-based ceramics. Various ...
In the present study nonoxide ceramic materials based on silicon nitride were evaluated with respect...
The oxidation behaviour of Y2O3 plus Al2O3-doped Si3N4 based ceramics was investigated in air up to ...
The oxidation behavior of polymer-derived amorphous SiAlCNs was studied in the temperature range of ...
The oxidation behavior of polymer-derived amorphous SiAlCNs was studied in the temperature range of ...
The oxidation behaviour of hot-pressed β-SiAlON ceramics with different densities has been investiga...
Sintered ceramics produced from two kinds of silicon nitride powder were oxidized at 1000 and 1400 d...
Structural ceramics are potential mold materials for hot embossing, due to their superior mechanical...
International audienceThe oxidation of a silicon nitride–titanium nitride ceramic has been studied. ...
The effect of oxidation on the room-temperature mechanical properties of silicon nitride ceramics wi...
International audienceThe rate of air oxidation towards 1,000degreesC of the Si3N4-bonded silicon ca...
Within this study, the oxidation behavior of SiHfBCN ceramic powders and monoliths was studied at te...
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
The oxidation kinetics of amorphous silicon carbonitride (SiCN) was measured at 1350°C in ambient a...
Within this study, the oxidation behavior of SiHfBCN ceramic powders and monoliths was studied at te...