Laser-based technology of direct metal deposition has matured into an industrially well established technique for precise coating deposition and additive manufacturing. By means of dedicated nozzle systems, suitable process equipment as well as well customized manufacturing strategies, the fabrication of miniaturized, but even very large components becomes feasible. This includes the use of powder as well as wire for the added material. Fostered by high demands, e. g. in the field of stationary gas turbines or jet engines, the state of the art has to be extended especially in the direction of lightweight fabrication as well as increased temperature performance of processed materials. However, from a materials perspective, these materials ar...
The present paper reviews recent progress in productivity, precision and quality of laser-based clad...
Laser-based additive manufacturing (AM) technologies such as laser metal deposition have been introd...
Laser Metal Deposition (LMD), an additive manufacturing technique, is described here as an alternate...
AbstractRecently, additive manufacturing is the one of most perspective technologies; it can replace...
Laser metal deposition has been already introduced in various industrial branches, as aviation, ener...
Laser metal deposition (LMD) has been already introduced in various industrial branches, as aviation...
Nickel-based superalloys are substantially used in the manufacturing of boilers for ultra-supercriti...
The present paper addresses the phenomena of hot cracking of nickel-based superalloys in the perspec...
In the meantime, laser-based deposition of metallic material in form of powder or wire became a well...
Laser additive direct deposition of metals is a new rapid manufacturing technology, which combines w...
Laser additive direct deposition of metals is a new rapid manufacturing technology, which combines w...
The subject of repairing Ni-based parts with state-of-the-art technologies is increasingly addressed...
The subject of repairing Ni-based parts with state-of-the-art technologies is increasingly addressed...
Laser metal deposition (LMD) is an established technology for two-dimensional surface coatings. It o...
Paper presents results of laser additive manufacturing. Deposition of nickel based super alloy Incon...
The present paper reviews recent progress in productivity, precision and quality of laser-based clad...
Laser-based additive manufacturing (AM) technologies such as laser metal deposition have been introd...
Laser Metal Deposition (LMD), an additive manufacturing technique, is described here as an alternate...
AbstractRecently, additive manufacturing is the one of most perspective technologies; it can replace...
Laser metal deposition has been already introduced in various industrial branches, as aviation, ener...
Laser metal deposition (LMD) has been already introduced in various industrial branches, as aviation...
Nickel-based superalloys are substantially used in the manufacturing of boilers for ultra-supercriti...
The present paper addresses the phenomena of hot cracking of nickel-based superalloys in the perspec...
In the meantime, laser-based deposition of metallic material in form of powder or wire became a well...
Laser additive direct deposition of metals is a new rapid manufacturing technology, which combines w...
Laser additive direct deposition of metals is a new rapid manufacturing technology, which combines w...
The subject of repairing Ni-based parts with state-of-the-art technologies is increasingly addressed...
The subject of repairing Ni-based parts with state-of-the-art technologies is increasingly addressed...
Laser metal deposition (LMD) is an established technology for two-dimensional surface coatings. It o...
Paper presents results of laser additive manufacturing. Deposition of nickel based super alloy Incon...
The present paper reviews recent progress in productivity, precision and quality of laser-based clad...
Laser-based additive manufacturing (AM) technologies such as laser metal deposition have been introd...
Laser Metal Deposition (LMD), an additive manufacturing technique, is described here as an alternate...