Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on silicon (100) substrates. Progressive infilling of the air spaces within the structure with GaAs was achieved using trimethylgallium and arsine under atomic-layer-deposition conditions. Samples with the highest levels of GaAs infill were subsequently inverted using selective etching. Reflectance spectra are interpreted via the Bragg expression and calculated photonic band structure diagrams. For GaAs infilled and inverted samples, the relative positions of the first and second order Bragg reflections are strongly influenced by the wavelength dependent refractive index
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
The authors experimentally investigate the effects of atomic layer deposition (ALD) and laser-assist...
Photonic crystals (PC's) are emerging as potentially important candidates in propelling the developm...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
The past decade and a half has seen the rapid emergence of a new material class known as photonic cr...
In the late eighties, a new class of materials, known as photonic crystals (PCs), emerged enabling t...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
[[abstract]]We propose a method for forming a top distributed Bragg reflector (DBR) during very-low ...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
The authors experimentally investigate the effects of atomic layer deposition (ALD) and laser-assist...
Photonic crystals (PC's) are emerging as potentially important candidates in propelling the developm...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
Photonic crystal thin films were fabricated via the self-assembly of a lattice of silica spheres on ...
The past decade and a half has seen the rapid emergence of a new material class known as photonic cr...
In the late eighties, a new class of materials, known as photonic crystals (PCs), emerged enabling t...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Atomic layer deposition (ALD) has become a powerful tool for the fabrication of high quality 3-dimen...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
[[abstract]]We propose a method for forming a top distributed Bragg reflector (DBR) during very-low ...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
Opals consist of an ordered array of SiO2 spheres. This leads to a modulation of the refractive inde...
The authors experimentally investigate the effects of atomic layer deposition (ALD) and laser-assist...
Photonic crystals (PC's) are emerging as potentially important candidates in propelling the developm...