International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed laser deposition on SrTiO 3 using combinatorial substrate epitaxy (CSE) approach, i.e. polycrystalline substrates with micrometer-size grains. The crystallographic domains size of those polycrystalline substrates can be controlled between 2 and 45 µ m depending on the annealing temperature during synthesis. Each grain of the substrate acts as a single crystalline growth template promoting local epitaxy with a reproduction of the substrate grain structure in the thin film. Therefore, a fine-tuning of the substrate grain metrics and high crystalline quality of locally epitaxial LSMO film, allows to combine the advantages of polycrystalline, i.e. t...
We have grown La{sub 1-x}Sr{sub x}MnO{sub 3} films, using both pulsed laser deposition and a polymer...
We report a comparative study of the magnetoelectrical properties of epitaxial and polycrystalline t...
Nearly 50-nm thick La 0.7 Sr 0.3 MnO 3 (LSMO) films were grown on Si substrates using molecular beam...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
Nearly 50-nm thick La 0.7 Sr 0.3 MnO 3 (LSMO) films were grown on Si substrates using molecular beam...
We have grown La{sub 1-x}Sr{sub x}MnO{sub 3} films, using both pulsed laser deposition and a polymer...
We report a comparative study of the magnetoelectrical properties of epitaxial and polycrystalline t...
Nearly 50-nm thick La 0.7 Sr 0.3 MnO 3 (LSMO) films were grown on Si substrates using molecular beam...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceAbstract La 0.67 Sr 0.33 MnO 3 (LSMO) thin films have been grown by pulsed las...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
International audienceLa0.67Sr0.33MnO3 (LSMO) thin films have been grown by pulsed laser deposition ...
Nearly 50-nm thick La 0.7 Sr 0.3 MnO 3 (LSMO) films were grown on Si substrates using molecular beam...
We have grown La{sub 1-x}Sr{sub x}MnO{sub 3} films, using both pulsed laser deposition and a polymer...
We report a comparative study of the magnetoelectrical properties of epitaxial and polycrystalline t...
Nearly 50-nm thick La 0.7 Sr 0.3 MnO 3 (LSMO) films were grown on Si substrates using molecular beam...