Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed dislocation pile-up and transmission across the boundary. The latter is observed as a characteristic displacement jump, from which the Hall-Petch slope can be calculated as a measure for the slip transmission properties of the boundary. (C) 2005 Elsevier B.V. All rights reserved.</p
© 2018, Springer Science+Business Media, LLC, part of Springer Nature. Nanoindentation experiments a...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation was undertaken near grain boundaries to increase understanding of their individual c...
The influence of grain boundaries on material deformation in Ni3Al was investigated by relating the ...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoindentation near grain boundaries has been investigated in an Fe–14%S...
© 2018, Springer Science+Business Media, LLC, part of Springer Nature. Nanoindentation experiments a...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation measurements near a high-angle grain boundary in a Fe-14%Si bicrystal showed disloca...
Nanoindentation was undertaken near grain boundaries to increase understanding of their individual c...
The influence of grain boundaries on material deformation in Ni3Al was investigated by relating the ...
The mechanical response to nanoinclentation near grain boundaries has been investigated in an Fe-14%...
The mechanical response to nanoindentation near grain boundaries has been investigated in an Fe–14%S...
© 2018, Springer Science+Business Media, LLC, part of Springer Nature. Nanoindentation experiments a...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...
In this paper, it is shown'that the occurrence of dislocation pileups across grain boundaries, as we...