The inhibition of Stress Corrosion Cracking (SCC) of AISI 316S stainless steel (SS) in 2 N HCl solution by aromatic and heterocyclic substances has been studied. The evaluation of the inhibitors in reducing SCC of U-bend SS specimens has been carried out by micrographic measurements. The registration of anodic and cathodic polarization curves shows that the inhibiting action towards SCC is related to the effects the organic compounds exert on the anodic dissolution process of the alloys. An interpretation of SCC in HCl solution is hypothesized involving an adsorbed layer of chloride ions. Tests performed with scratched electrodes seem to confirm the proposed interpretation
The stress corrosion behavior of AISI Type 304L stainless steel has been investigated in H_2SO_4/NaC...
Department of Chemistry, Patna University, Patna-800 005, Bihar, India Manuscript received 28 June ...
The effect of different anions (bicarbonate, phosphate, sulphate, hydroxyl) on the pitting corrosion...
The application of a scratching electrode technique has been developed to obtain further information...
A Slow Strain Rate (1x10e-6 s-1) has been applied to study the possibility of inhibiting or delaying...
The efficiency of some organic additives for SCC inhibition of AISI 304 SS in 1 M HCl can be demonst...
The inhibiting effect of some organic compounds at 0.1 mM concentration on the stress corrosion crac...
The inhibition of Stress Corrosion Cracking (SCC) of austenitic stainless steel wires in boiling (13...
This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC)...
The slow strain rate testing technique was used to study the stress cor-rosion cracking (SCC) suscep...
Stress corrosion cracking (SCC) of type 316 stainless steel was studied in hot (92°C) solutions of 3...
Some different types of organic substances (an acetylenic derivative, S- or N-containing compounds) ...
Source: Dissertation Abstracts International, Volume: 39-02, Section: B, page: 7750.Ph.D. American U...
Some organic inhibitors of steel corrosion in saturated calcium hydroxide solutions containing 0.1 M...
International audienceThe effect of certain non-toxic inhibitors on the corrosion resistance of ordi...
The stress corrosion behavior of AISI Type 304L stainless steel has been investigated in H_2SO_4/NaC...
Department of Chemistry, Patna University, Patna-800 005, Bihar, India Manuscript received 28 June ...
The effect of different anions (bicarbonate, phosphate, sulphate, hydroxyl) on the pitting corrosion...
The application of a scratching electrode technique has been developed to obtain further information...
A Slow Strain Rate (1x10e-6 s-1) has been applied to study the possibility of inhibiting or delaying...
The efficiency of some organic additives for SCC inhibition of AISI 304 SS in 1 M HCl can be demonst...
The inhibiting effect of some organic compounds at 0.1 mM concentration on the stress corrosion crac...
The inhibition of Stress Corrosion Cracking (SCC) of austenitic stainless steel wires in boiling (13...
This article describes the susceptibility of 316L stainless steel to stress corrosion cracking (SCC)...
The slow strain rate testing technique was used to study the stress cor-rosion cracking (SCC) suscep...
Stress corrosion cracking (SCC) of type 316 stainless steel was studied in hot (92°C) solutions of 3...
Some different types of organic substances (an acetylenic derivative, S- or N-containing compounds) ...
Source: Dissertation Abstracts International, Volume: 39-02, Section: B, page: 7750.Ph.D. American U...
Some organic inhibitors of steel corrosion in saturated calcium hydroxide solutions containing 0.1 M...
International audienceThe effect of certain non-toxic inhibitors on the corrosion resistance of ordi...
The stress corrosion behavior of AISI Type 304L stainless steel has been investigated in H_2SO_4/NaC...
Department of Chemistry, Patna University, Patna-800 005, Bihar, India Manuscript received 28 June ...
The effect of different anions (bicarbonate, phosphate, sulphate, hydroxyl) on the pitting corrosion...