The microstructure of Al-Si-Mg alloys strongly depends on their chemical composition and the heat treatment they undergo during production. The influence of solution heat treatment (SHT) and the addition of Er and Zr on the microstructure of gravity-cast A356 (Al-7Si-0.4Mg) were examined. The reference as-cast microstructure is characterized by the grain size and morphology of eutectic Si, as well as the morphology, area fraction, and chemical composition of the intermetallic compounds. The morphology of eutectic Si is unstable during SHT; the evolution mechanisms can be described using thermodynamic and kinetic models and have been validated using optical and scanning electron microscope (SEM) micrographs. The effect of high-temperature ex...