Electrospun polymeric nanofibers were either surface-decorated with zinc oxide (ZnO) nanoparticles or coated with a continuous ZnO thin film with a precise thickness (∼27 nm) via atomic layer deposition (ALD) for the fabrication of flexible photocatalytic nanofibrous membranes. © 2013 The Royal Society of Chemistry
This study is focused on forming a spider-wave-like nano-nets of nylon-6 decorated with unique mop-b...
Free-standing and highly interconnected ZnO tubes consisting of nanostructured single phase grains a...
A simple and efficient method has been developed for preparing hierarchical nanostructures of polyim...
Cataloged from PDF version of article.Electrospun polymeric nanofibers were either surface-decorated...
Organic-inorganic core-shell nanofibers were fabricated by combining electrospinning and atomic laye...
A hierarchy of nanostructured-ZnO was fabricated on the electrospun nanofibers by atomic layer depos...
In this study, the best conditions to obtain Zinc Oxide (ZnO) nanofibers were studied for further de...
Abstract: The unique combination of optical, chemical, and structural properties of one-dimensional ...
The present research is focused on the synthesis of hexagonal ZnO wurtzite nanorods for the decorati...
We report on the synthesis and photocatalytic activity (PCA) of electrospun poly(acrylonitrile) (PAN...
Cataloged from PDF version of article.We report on the synthesis and photocatalytic activity (PCA) o...
AbstractNanometer (nm) scale 1D zinc oxide (ZnO) nanofibers were fabricated through sol–gel processi...
none7noWe present a two-step process to obtain PMMA fibrous membranes with homogeneously in situ syn...
Fabrication and decoration of flexible Nylon 6,6 polymeric nanofibrous mats for production of multif...
Orientadores: Ana Rita Morales, Renato Carajelescov NonatoDissertação (mestrado) - Universidade Esta...
This study is focused on forming a spider-wave-like nano-nets of nylon-6 decorated with unique mop-b...
Free-standing and highly interconnected ZnO tubes consisting of nanostructured single phase grains a...
A simple and efficient method has been developed for preparing hierarchical nanostructures of polyim...
Cataloged from PDF version of article.Electrospun polymeric nanofibers were either surface-decorated...
Organic-inorganic core-shell nanofibers were fabricated by combining electrospinning and atomic laye...
A hierarchy of nanostructured-ZnO was fabricated on the electrospun nanofibers by atomic layer depos...
In this study, the best conditions to obtain Zinc Oxide (ZnO) nanofibers were studied for further de...
Abstract: The unique combination of optical, chemical, and structural properties of one-dimensional ...
The present research is focused on the synthesis of hexagonal ZnO wurtzite nanorods for the decorati...
We report on the synthesis and photocatalytic activity (PCA) of electrospun poly(acrylonitrile) (PAN...
Cataloged from PDF version of article.We report on the synthesis and photocatalytic activity (PCA) o...
AbstractNanometer (nm) scale 1D zinc oxide (ZnO) nanofibers were fabricated through sol–gel processi...
none7noWe present a two-step process to obtain PMMA fibrous membranes with homogeneously in situ syn...
Fabrication and decoration of flexible Nylon 6,6 polymeric nanofibrous mats for production of multif...
Orientadores: Ana Rita Morales, Renato Carajelescov NonatoDissertação (mestrado) - Universidade Esta...
This study is focused on forming a spider-wave-like nano-nets of nylon-6 decorated with unique mop-b...
Free-standing and highly interconnected ZnO tubes consisting of nanostructured single phase grains a...
A simple and efficient method has been developed for preparing hierarchical nanostructures of polyim...