Hot deformation of cast-homogenized and extruded (in both the extrusion and transverse directions) ZK60 magnesium alloy was conducted using the Gleeble® 3500 thermal-mechanical simulation testing system. A new approach to model the high temperature constitutive behavior of the alloy was done using two well-known equations (i.e. hyperbolic sine and Ludwig equations). For this approach, the deformation conditions were divided into regimes of low and high temperature and strain rate (four regimes). Constitutive model development was conducted in each regime and the material parameters (P) were evaluated as strain, strain rate and temperature-dependent variables; P(ε, ε˙, T). Using this approach, the flow curves were predicted with high accurac...
The high temperature forming behavior of WE54 magnesium alloy is studied by means of compression and...
AbstractDue to their hexagonal crystal structure, magnesium alloys have relatively low workability a...
The characteristics of constitutive behavior and microstructure evolution of GW103K magnesium alloy ...
The hot deformation behavior of T4-treated ZK60 magnesium alloy was investigated in a compression te...
Isothermal warm and hot deformation behavior of as-cast ZEK100 (Mg-1.2Zn-0.25Zr-0.17Nd, in wt.%) mag...
Forgeability of as-cast ZK60 magnesium alloy was investigated by isothermal uniaxial hot compression...
The hot deformation behavior of an AZ81 magnesium alloy was investigated by hot compressive testing ...
Hot compression tests were conducted on the as-extruded ZK60 magnesium alloy in both extrusion and t...
AbstractIn this study, the hyperbolic-sine type constitutive equation was used to model the flow str...
Hot deformation behaviors of a ZK60 magnesium alloy were investigated by hot compressive tests on a ...
The present study investigates the variation of flow stress and microstructural evolution with strai...
The present study aimed at characterizing the flow characteristics and workability of an as-extruded...
The thermal deformation behaviour of Mg-9Gd-4Y-2Zn-0.5Zr alloy at temperatures of 360–480 °C, strain...
The Gleeble-3500 thermal simulation tester was used to perform hot deformation behavior on the extru...
In order to understand the constitutive behavior of as-cast AZ80 with large grain size, the uniaxial...
The high temperature forming behavior of WE54 magnesium alloy is studied by means of compression and...
AbstractDue to their hexagonal crystal structure, magnesium alloys have relatively low workability a...
The characteristics of constitutive behavior and microstructure evolution of GW103K magnesium alloy ...
The hot deformation behavior of T4-treated ZK60 magnesium alloy was investigated in a compression te...
Isothermal warm and hot deformation behavior of as-cast ZEK100 (Mg-1.2Zn-0.25Zr-0.17Nd, in wt.%) mag...
Forgeability of as-cast ZK60 magnesium alloy was investigated by isothermal uniaxial hot compression...
The hot deformation behavior of an AZ81 magnesium alloy was investigated by hot compressive testing ...
Hot compression tests were conducted on the as-extruded ZK60 magnesium alloy in both extrusion and t...
AbstractIn this study, the hyperbolic-sine type constitutive equation was used to model the flow str...
Hot deformation behaviors of a ZK60 magnesium alloy were investigated by hot compressive tests on a ...
The present study investigates the variation of flow stress and microstructural evolution with strai...
The present study aimed at characterizing the flow characteristics and workability of an as-extruded...
The thermal deformation behaviour of Mg-9Gd-4Y-2Zn-0.5Zr alloy at temperatures of 360–480 °C, strain...
The Gleeble-3500 thermal simulation tester was used to perform hot deformation behavior on the extru...
In order to understand the constitutive behavior of as-cast AZ80 with large grain size, the uniaxial...
The high temperature forming behavior of WE54 magnesium alloy is studied by means of compression and...
AbstractDue to their hexagonal crystal structure, magnesium alloys have relatively low workability a...
The characteristics of constitutive behavior and microstructure evolution of GW103K magnesium alloy ...