The creep behaviour of injection moulded PA 6/organoclay nanocomposites was studied by depth-sensing nanoindentation and DMA cantilever-bending. The glass transitions of PA 6 and its nanocomposites were decreased below room temperature upon saturation with water so that the materials could be tested in the rubbery regime. For nanoindentation creep on the skin and core regions of injection moulded samples, whilst organoclay improves the creep resistance of PA 6, the enhancement is due to the decrease of the initial compliance at zero time but the time-dependent creep is actually increased. In contrast, for cantilever-bending creep, organoclay reduces the creep compliance and the time-dependent creep in PA 6. It is suggested that the organocl...
Polymer nanocomposites and their behavior have been widely investigated by several paths, including ...
The study is devoted to prediction of elastic and creep properties of thermoplastic polymer nanocomp...
International audienceThe polyamide 6 (PA6) under study exhibits non-linear time dependent (viscopla...
general discussions on the creep resistance of polyamide 66 nanocomposites. To promote these works, ...
[[abstract]]Nanocomposites of polyamide six (PA6) reinforced with organoclay were prepared in this s...
International audienceThe influence of the incorporation of nanoparticles (organo-modified montmoril...
The effect of water immersion on the morphology and indentation modulus of injection moulded nylon 6...
In the present study, one of the unique improvements in polymer nanocomposites has been detected. On...
In this study, we report that a synergistic effect exists in the surface mechanical properties of ny...
It has been found, in this study, that there is no close correlation between the tensile and nanoind...
A series of exfoliated and intercalated polyurethane organoclay nanocomposites were prepared by in s...
Abstract: The nanoindentation creep behaviour of several different polymers has been investigated. T...
Creep can be understood as the resistance of a material to a continuous stress and represents an imp...
ABSTRACT: This article investigates the effect of moisture on the dynamic mechanical behavior of pol...
This paper describes investigations on dynamic mechanical analysis (DMA) of nylon 6,6 thermoplastic ...
Polymer nanocomposites and their behavior have been widely investigated by several paths, including ...
The study is devoted to prediction of elastic and creep properties of thermoplastic polymer nanocomp...
International audienceThe polyamide 6 (PA6) under study exhibits non-linear time dependent (viscopla...
general discussions on the creep resistance of polyamide 66 nanocomposites. To promote these works, ...
[[abstract]]Nanocomposites of polyamide six (PA6) reinforced with organoclay were prepared in this s...
International audienceThe influence of the incorporation of nanoparticles (organo-modified montmoril...
The effect of water immersion on the morphology and indentation modulus of injection moulded nylon 6...
In the present study, one of the unique improvements in polymer nanocomposites has been detected. On...
In this study, we report that a synergistic effect exists in the surface mechanical properties of ny...
It has been found, in this study, that there is no close correlation between the tensile and nanoind...
A series of exfoliated and intercalated polyurethane organoclay nanocomposites were prepared by in s...
Abstract: The nanoindentation creep behaviour of several different polymers has been investigated. T...
Creep can be understood as the resistance of a material to a continuous stress and represents an imp...
ABSTRACT: This article investigates the effect of moisture on the dynamic mechanical behavior of pol...
This paper describes investigations on dynamic mechanical analysis (DMA) of nylon 6,6 thermoplastic ...
Polymer nanocomposites and their behavior have been widely investigated by several paths, including ...
The study is devoted to prediction of elastic and creep properties of thermoplastic polymer nanocomp...
International audienceThe polyamide 6 (PA6) under study exhibits non-linear time dependent (viscopla...