This paper provides an analysis of experimental research and results of investment casting process. Temperature field in a ceramic mold is one of the problems during numerical simulation. Reducing the costs of production in precision casting involves the reduction of scraps, which is one of the fundamental problems of the foundry industry. Reducing these costs is associated with optimization of precision casting technology of aircraft engines critical parts, including control of the solidification front in thin-walled castings of nickel super alloys cast in a vacuum. It is achieved by changing the geometrical characteristics of the ceramic mold. The results of the tests were used to optimize the industrial production of aircraft components ...
International audienceA process model is described for the grain selection occurring during the soli...
The paper presents the results of research on the determination of the effect of pouring temperature...
A mathematical model based on the control volume method with fixed mesh was selected in order to sim...
This paper provides an analysis of experimental research and results of investment casting process. ...
Components for engineering systems, such as gas turbines and jet engines operating at high temperatu...
The paper presents the method of manufacturing casts made of the IN-713C nickel superalloy using the...
The analysis of influence of mould withdrawal rate on the solidification process of CMSX-4 single cr...
In order to automate the vacuum induction melting of B1900 nickel-based superalloys, a procedure tha...
Manufacturing processes are getting more and more complex with increasing demands of advanced and li...
Accelerating advancements in technological systems have demonstrated a need for alloys with drastica...
Thesis submitted in fulfilment of the requirements for the degree Master of Technology: Mechanical E...
Heat transfer during metal pouring and its solidification in the vacuum furnace have been investigat...
The paper presents the results concerning impact of modification (volume and surface techniques), po...
The use of rapid prototyping technologies provides a unique opportunity of cost-effective methods of...
AbstractThis paper presents the adjustment process of a simulation model to improve the correlation ...
International audienceA process model is described for the grain selection occurring during the soli...
The paper presents the results of research on the determination of the effect of pouring temperature...
A mathematical model based on the control volume method with fixed mesh was selected in order to sim...
This paper provides an analysis of experimental research and results of investment casting process. ...
Components for engineering systems, such as gas turbines and jet engines operating at high temperatu...
The paper presents the method of manufacturing casts made of the IN-713C nickel superalloy using the...
The analysis of influence of mould withdrawal rate on the solidification process of CMSX-4 single cr...
In order to automate the vacuum induction melting of B1900 nickel-based superalloys, a procedure tha...
Manufacturing processes are getting more and more complex with increasing demands of advanced and li...
Accelerating advancements in technological systems have demonstrated a need for alloys with drastica...
Thesis submitted in fulfilment of the requirements for the degree Master of Technology: Mechanical E...
Heat transfer during metal pouring and its solidification in the vacuum furnace have been investigat...
The paper presents the results concerning impact of modification (volume and surface techniques), po...
The use of rapid prototyping technologies provides a unique opportunity of cost-effective methods of...
AbstractThis paper presents the adjustment process of a simulation model to improve the correlation ...
International audienceA process model is described for the grain selection occurring during the soli...
The paper presents the results of research on the determination of the effect of pouring temperature...
A mathematical model based on the control volume method with fixed mesh was selected in order to sim...