International audienceTribochemical properties are an essential component of the efficiency of metal forming lubricants. Their understanding, a basis for the selection of adequate additives, heavily relies on surface analytical techniques. In the last ten years, we have applied time-of-flight secondary ion mass spectroscopy (ToF-SIMS) to the analysis of the reactions of strip surfaces with typical additives of cold strip rolling and deep drawing lubricants. Data analysis procedures have been evolved to perform semi-quantitative comparisons. Analytical results performed on laboratory simulation tests and on real-size processes are compared. Examples of competition and synergies between different additives in a single lubricant are describe
\u3cp\u3eIn the last few years static secondary ion mass spectrometry (SSIMS) has proved to be a ver...
The potential applicability of time-of-flight secondary ion mass spectrometry (ToF SIMS) as an indep...
International audienceControlling and predicting the tribological behavior of dry lubricants is a ne...
Boundary lubricating behaviors were investigated from the viewpoint of surface chemistry based on ou...
Time-of-Flight Secondary Ion Mass Spectrometry (ToF-SIMS) is a powerful tool for investigating the e...
In recent years, time of flight-secondary ion mass spectrometer (ToF-SIMS) has been widely employed ...
This paper provides a critical review on the applications of time-of-flight secondary ion mass spect...
Progress in analytical spectroscopic methods and in the instrumentation for tribological measurement...
High-density polyethylene (HDPE) and polypropylene (PP) films were analysed by time-of-flight second...
Static secondary ion mass spectrometry was used to study the chemical reactions and lateral distribu...
Time-of-flight secondary ion mass spectrometry (ToF-SIMS) is a powerful analytical technique with gr...
La Spectrométrie de Masse d'Ions Secondaires à Temps de Vol (ToF-SIMS) permet la caractérisation de ...
The surface chemistry of starch-coated fine and LWC papers was studied using Time-of-Flight Secondar...
Antagonistic effect on lubricity of overbased calcium sulfonate by zine dialkyldithiophosphate(ZnDTP...
International audienceAn experimental investigation of the tribology during plane strain compression...
\u3cp\u3eIn the last few years static secondary ion mass spectrometry (SSIMS) has proved to be a ver...
The potential applicability of time-of-flight secondary ion mass spectrometry (ToF SIMS) as an indep...
International audienceControlling and predicting the tribological behavior of dry lubricants is a ne...
Boundary lubricating behaviors were investigated from the viewpoint of surface chemistry based on ou...
Time-of-Flight Secondary Ion Mass Spectrometry (ToF-SIMS) is a powerful tool for investigating the e...
In recent years, time of flight-secondary ion mass spectrometer (ToF-SIMS) has been widely employed ...
This paper provides a critical review on the applications of time-of-flight secondary ion mass spect...
Progress in analytical spectroscopic methods and in the instrumentation for tribological measurement...
High-density polyethylene (HDPE) and polypropylene (PP) films were analysed by time-of-flight second...
Static secondary ion mass spectrometry was used to study the chemical reactions and lateral distribu...
Time-of-flight secondary ion mass spectrometry (ToF-SIMS) is a powerful analytical technique with gr...
La Spectrométrie de Masse d'Ions Secondaires à Temps de Vol (ToF-SIMS) permet la caractérisation de ...
The surface chemistry of starch-coated fine and LWC papers was studied using Time-of-Flight Secondar...
Antagonistic effect on lubricity of overbased calcium sulfonate by zine dialkyldithiophosphate(ZnDTP...
International audienceAn experimental investigation of the tribology during plane strain compression...
\u3cp\u3eIn the last few years static secondary ion mass spectrometry (SSIMS) has proved to be a ver...
The potential applicability of time-of-flight secondary ion mass spectrometry (ToF SIMS) as an indep...
International audienceControlling and predicting the tribological behavior of dry lubricants is a ne...