International audienceThe relationships between heat treatment parameters and microstructure, and between microstructure and mechanical properties were investigated in the SMO43 disc P/M superalloy. Various heat treatments were applied to this superalloy to determine the effect of the solution temperature on the grain size, and of the cooling path and aging temperature on the ' precipitates distribution. Microstructural features were characterised through the careful study of ' precipitation. Fatigue crack growth tests with dwell time were performed at high temperature for comparison of the mechanical properties of some selected microstructures
The effect of heat treatments on the microstructure and mechanical properties of Ni base superalloys...
AbstractThe nickel base superalloy, supercast 247A gains its appropriate microstructure and high tem...
The effect of solution treatment and intermediate heat treatment on the microstructure and propertie...
L'alliage N19 est un superalliage base nickel, élaboré par métallurgie des poudres, qui a été dévelo...
The N19 alloy is a powder metallurgy nickel-based superalloy which has recently been developed for a...
The enhancement of efficiency in power generation gas turbine requires the development of new supera...
The enhancement of efficiency in power generation gas turbine requires the development of new supera...
Nickel-based alloy like N18 can present various types of precipitate distributions according to the ...
PER72® is a nickel-base superalloys developed by Aubert & Duval. This alloy is used in helicopter en...
Compte tenu de l’évolution des températures d’entrée de turbines, le principal enjeu pour les métall...
The fabrication of gamma prime (γ′) strengthened nickel-based superalloys by additive manufacturing ...
Microstructures of the new PM superalloy N19 have been investigated for various heat treatments in o...
The microstructure and fatigue performance of three sub-solvus heat treated nickel based disc supera...
The effect of heat treatment on the microstructure and mechanical properties of Ni-base superalloy H...
Nickel-based superalloys are distinguished from other materials by their excellent mechanical and ph...
The effect of heat treatments on the microstructure and mechanical properties of Ni base superalloys...
AbstractThe nickel base superalloy, supercast 247A gains its appropriate microstructure and high tem...
The effect of solution treatment and intermediate heat treatment on the microstructure and propertie...
L'alliage N19 est un superalliage base nickel, élaboré par métallurgie des poudres, qui a été dévelo...
The N19 alloy is a powder metallurgy nickel-based superalloy which has recently been developed for a...
The enhancement of efficiency in power generation gas turbine requires the development of new supera...
The enhancement of efficiency in power generation gas turbine requires the development of new supera...
Nickel-based alloy like N18 can present various types of precipitate distributions according to the ...
PER72® is a nickel-base superalloys developed by Aubert & Duval. This alloy is used in helicopter en...
Compte tenu de l’évolution des températures d’entrée de turbines, le principal enjeu pour les métall...
The fabrication of gamma prime (γ′) strengthened nickel-based superalloys by additive manufacturing ...
Microstructures of the new PM superalloy N19 have been investigated for various heat treatments in o...
The microstructure and fatigue performance of three sub-solvus heat treated nickel based disc supera...
The effect of heat treatment on the microstructure and mechanical properties of Ni-base superalloy H...
Nickel-based superalloys are distinguished from other materials by their excellent mechanical and ph...
The effect of heat treatments on the microstructure and mechanical properties of Ni base superalloys...
AbstractThe nickel base superalloy, supercast 247A gains its appropriate microstructure and high tem...
The effect of solution treatment and intermediate heat treatment on the microstructure and propertie...