The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activated in a high-energy planetary mill for 15 min and then sintered between 800 and 1100 degrees C for 2 h. The influence of MgO addition on the structure of the samples obtained is analyzed with X-ray diffraction and infrared reflection spectroscopy. Room-temperature far-infrared reflectivity spectra of the samples doped with MgO (0, 1.25, and 2.5 wt.%) and sintered at 1100 degrees C in the frequency range between 100 and 1200 cm(-1) are measured and analyzed. Optical parameters are determined for seven oscillators belonging to the spinel structure using the four-parameter model of coupled oscillators. Born effective charges are calculated from ...
In this article the influence of ball miling process on structure of MgO-TiO2 system, as well as the...
A mixture of starting ZnO and SnO2 powders (molar ratio 2: 1) were mechanically activated for 10, 40...
In this article the influence of ball miling process on structure of MgO–TiO2 system, as well as the...
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activat...
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mil...
The aim of this work was analysis of isothermal sintering of zinc titanate ceramics doped with MgO o...
The aim of this work is to analyze nonisothermal sintering of zinc titanate ceramics doped with MgO ...
International audienceWe report on optical and structural investigations of Mn4+ activated (ZnxMg1-x...
Starting mixtures of ZnO, TiO(2) and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activa...
Poster presented at the Fizika i tehnologija materijala (Physics and Technology of Materials), FITEM...
In this article the influence of ball miling process on structure of MgO-TiO2 system, as well as the...
A mixture of starting ZnO and SnO2 powders (molar ratio 2: 1) were mechanically activated for 10, 40...
In this article the influence of ball miling process on structure of MgO–TiO2 system, as well as the...
The starting mixtures of ZnO, TiO2, and MgO (0, 1.25, and 2.5 wt.%) powders are mechanically activat...
Zinc-titanate ceramics were obtained by initial mechanical activation in a high-energy planetary mil...
The aim of this work was analysis of isothermal sintering of zinc titanate ceramics doped with MgO o...
The aim of this work is to analyze nonisothermal sintering of zinc titanate ceramics doped with MgO ...
International audienceWe report on optical and structural investigations of Mn4+ activated (ZnxMg1-x...
Starting mixtures of ZnO, TiO(2) and MgO (0, 1.25 and 2.5 wt.% MgO) powders were mechanically activa...
Poster presented at the Fizika i tehnologija materijala (Physics and Technology of Materials), FITEM...
In this article the influence of ball miling process on structure of MgO-TiO2 system, as well as the...
A mixture of starting ZnO and SnO2 powders (molar ratio 2: 1) were mechanically activated for 10, 40...
In this article the influence of ball miling process on structure of MgO–TiO2 system, as well as the...