This study develops a three-dimensional automated detection framework (PitScan) that systematically evaluates the severity and phenomenology of pitting corrosion. This framework uses a python-based algorithm to analyse microcomputer-tomography scans (μCT) of cylindrical specimens undergoing corrosion. The approach systematically identifies several surface-based corrosion features, enabling full spatial characterisation of pitting parameters, including pit density, pit size, pit depth as well as pitting factor according to ASTM G46-94. Furthermore, it is used to evaluate pitting formation in tensile specimens of a Rare Earth Magnesium alloy undergoing corrosion, and relationships between key pitting parameters and mechanical performance are ...
Pitting corrosion is an insidious form of localized corrosion affecting characteristics of various e...
This study experimentally investigated the effect of corrosion non-uniformity on the mechanical prop...
Aluminum alloy is widely used in aerospace structures. However, it often suffers from a harsh corros...
This study developed an enhanced phenomenological model for the predictions of surface-based localis...
abstract: Aluminum alloys are commonly used for engineering applications due to their high strength ...
Galvanic corrosion of the magnesium alloys AZ91D and AM60B combined with different coatings on steel...
This study adopts three-dimensional scanning technology to obtain accurate pit corrosion data to res...
A digital image processing and analysis method has been developed to classify shape and evaluate siz...
Corrosion is an ongoing problem till date. Lots of attention has been given to it as it has already ...
Pitting corrosion damage often occurs in aluminum alloy structures and can significantly reduce the ...
In this study, a new consistent formulation coupling kinematics, thermodynamics, and kinetics with d...
The article of record as published may be found at https://doi.org/10.3390/met10050651Magnesium is a...
The article shows that the use of quantitative fracture description may lead to significant progress...
Click on the DOI link to access the article (may not be free).Biodegradable materials including biod...
Raw data utilised to plot the graphs presented in the article. A combination of potentiostatic and p...
Pitting corrosion is an insidious form of localized corrosion affecting characteristics of various e...
This study experimentally investigated the effect of corrosion non-uniformity on the mechanical prop...
Aluminum alloy is widely used in aerospace structures. However, it often suffers from a harsh corros...
This study developed an enhanced phenomenological model for the predictions of surface-based localis...
abstract: Aluminum alloys are commonly used for engineering applications due to their high strength ...
Galvanic corrosion of the magnesium alloys AZ91D and AM60B combined with different coatings on steel...
This study adopts three-dimensional scanning technology to obtain accurate pit corrosion data to res...
A digital image processing and analysis method has been developed to classify shape and evaluate siz...
Corrosion is an ongoing problem till date. Lots of attention has been given to it as it has already ...
Pitting corrosion damage often occurs in aluminum alloy structures and can significantly reduce the ...
In this study, a new consistent formulation coupling kinematics, thermodynamics, and kinetics with d...
The article of record as published may be found at https://doi.org/10.3390/met10050651Magnesium is a...
The article shows that the use of quantitative fracture description may lead to significant progress...
Click on the DOI link to access the article (may not be free).Biodegradable materials including biod...
Raw data utilised to plot the graphs presented in the article. A combination of potentiostatic and p...
Pitting corrosion is an insidious form of localized corrosion affecting characteristics of various e...
This study experimentally investigated the effect of corrosion non-uniformity on the mechanical prop...
Aluminum alloy is widely used in aerospace structures. However, it often suffers from a harsh corros...