© 2022 The Author(s). The effect of solution temperature on the aging hardening behavior of Al-15%Mg2Si(-1%Cu) alloys was studied by characterizing the precipitation behaviors of nano-precipitates. After the solution temperature rises from 520 °C to 550 °C, more solute atoms are available for precipitation, and the formation activation energies of precipitates (β'' and S) decrease. So the formation of β''/β' in Al-15%Mg2Si alloy and S in Al-15%Mg2Si-1%Cu alloy is accelerated at a solution temperature of 550 °C, which enhances the hardness and ultimate tensile strength (UTS) of the two alloys.National Natural Science Foundation of China (No. 52122409); Natural Science Foundation of Tianjin City (No. 20JCYBJC00950)
Effect of Ag addition on the age-hardening response and precipitate microstructure of the Al-3.0Mg-1...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The mechanical properties of age hardenable Al alloys depend strongly on the precipitate microstruct...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
Nine Al-(1-3)Mg-(0-0.4)Cu-0.15Si-0.25Mn (in wt%) alloys with potential applications in both packagin...
The influence of cold rolling and solution treatment on precipitation in Al-(1-3)Mg-0.25Mn-(0 0.4)Cu...
High-Si aluminum foundry alloys are an important material class for products with complex 3D geometr...
The influence of a solution treatment with a trace zirconium addition on the precipitation behavior ...
Hardness measurements and Three-Dimensional Atom Probe (3DAP) were used to characterize the early st...
The effects of 3%–50% pre-deformation following solution heat treatment on the age hardening of an A...
Transmission electron microscopy, differential scanning calorimetry and hardness tests have been use...
The effect of different thermo-mechanical treatments on the hardness of the 2024 (Al-Cu-Mg) alloy wa...
Al-Mg-Si aluminium alloy are characterized by excellent deformability, but mechanical properties are...
Al-Mg-Si alloys are heat treatable alloys in which strength is obtained by precipitation hardening. ...
The solidification-precipitation behavior of Al-Mg-Si multicomponent alloys has long been an absorbi...
Effect of Ag addition on the age-hardening response and precipitate microstructure of the Al-3.0Mg-1...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The mechanical properties of age hardenable Al alloys depend strongly on the precipitate microstruct...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
Nine Al-(1-3)Mg-(0-0.4)Cu-0.15Si-0.25Mn (in wt%) alloys with potential applications in both packagin...
The influence of cold rolling and solution treatment on precipitation in Al-(1-3)Mg-0.25Mn-(0 0.4)Cu...
High-Si aluminum foundry alloys are an important material class for products with complex 3D geometr...
The influence of a solution treatment with a trace zirconium addition on the precipitation behavior ...
Hardness measurements and Three-Dimensional Atom Probe (3DAP) were used to characterize the early st...
The effects of 3%–50% pre-deformation following solution heat treatment on the age hardening of an A...
Transmission electron microscopy, differential scanning calorimetry and hardness tests have been use...
The effect of different thermo-mechanical treatments on the hardness of the 2024 (Al-Cu-Mg) alloy wa...
Al-Mg-Si aluminium alloy are characterized by excellent deformability, but mechanical properties are...
Al-Mg-Si alloys are heat treatable alloys in which strength is obtained by precipitation hardening. ...
The solidification-precipitation behavior of Al-Mg-Si multicomponent alloys has long been an absorbi...
Effect of Ag addition on the age-hardening response and precipitate microstructure of the Al-3.0Mg-1...
In this study, Al-1.00 Mg-0.65 Si-0.24 Cu alloy was solution heat-treated, water-quenched, and then ...
The mechanical properties of age hardenable Al alloys depend strongly on the precipitate microstruct...