In this present work, we present an accumulated inelastic strain rate based methodology to predict creep fatigue life of two different superalloys i.e. Haynes 282 and IN 718. The evolution of differential strain rate during creep and fatigue respectively motivated the present work. As creep is the rate controlling damage process in creep fatigue interaction, present mean strain rate based approach considers creep strain rate as a kinetic variable controlling the process. The other variable considered for this approach is accumulative cyclic strain during Creep-fatigue interaction. Our prediction method is purely based upon a relative accumulation rate of creep and fatigue strain. This method correlates the creep fatigue life with rate of in...
AbstractLow cycle fatigue (LCF) and fatigue-creep tests were conducted under different dwell conditi...
The thesis is focused on clarifying fatigue damage mechanisms and fatigue-creep damage mechanisms of...
The creep-fatigue behaviour of two representative, commercial ODS (Oxide dispersion-Strengthened) Su...
Abstract: The creep properties derived from stress relaxation tests are compared to those from creep...
The study deals with the interaction of creep and high cycle fatigue of cast polycrystalline nickel-...
Strain-controlled continuous fatigue and creep–fatigue tests were carried out at 700 °C and 800 °C o...
A novel creep-fatigue life prediction model was deduced based on an expression of the strain energy ...
Ni-base superalloys are employed as structural materials for the most critical hot gas path componen...
The accumulation of creep-fatigue damage over time is the principal damage mechanism which will even...
In this paper the creep-fatigue (CF) and low cycle fatigue (LCF) properties of alloy 263 are conside...
Ni-based superalloys, such as alloy 263, have excellent creep strength at high temperatures due to p...
Most engineering components used in gas/steam turbines are exposed to a range of complex loading con...
A generalised constitutive description of deformation of engineering alloys that exhibit a dominant ...
A new accelerated creep assessment method to evaluate the creep performance of metals and alloys fro...
A new accelerated creep assessment method to evaluate the creep performance of metals and alloys fro...
AbstractLow cycle fatigue (LCF) and fatigue-creep tests were conducted under different dwell conditi...
The thesis is focused on clarifying fatigue damage mechanisms and fatigue-creep damage mechanisms of...
The creep-fatigue behaviour of two representative, commercial ODS (Oxide dispersion-Strengthened) Su...
Abstract: The creep properties derived from stress relaxation tests are compared to those from creep...
The study deals with the interaction of creep and high cycle fatigue of cast polycrystalline nickel-...
Strain-controlled continuous fatigue and creep–fatigue tests were carried out at 700 °C and 800 °C o...
A novel creep-fatigue life prediction model was deduced based on an expression of the strain energy ...
Ni-base superalloys are employed as structural materials for the most critical hot gas path componen...
The accumulation of creep-fatigue damage over time is the principal damage mechanism which will even...
In this paper the creep-fatigue (CF) and low cycle fatigue (LCF) properties of alloy 263 are conside...
Ni-based superalloys, such as alloy 263, have excellent creep strength at high temperatures due to p...
Most engineering components used in gas/steam turbines are exposed to a range of complex loading con...
A generalised constitutive description of deformation of engineering alloys that exhibit a dominant ...
A new accelerated creep assessment method to evaluate the creep performance of metals and alloys fro...
A new accelerated creep assessment method to evaluate the creep performance of metals and alloys fro...
AbstractLow cycle fatigue (LCF) and fatigue-creep tests were conducted under different dwell conditi...
The thesis is focused on clarifying fatigue damage mechanisms and fatigue-creep damage mechanisms of...
The creep-fatigue behaviour of two representative, commercial ODS (Oxide dispersion-Strengthened) Su...