Poloxamers F88 (EO97PO39EO97) and P85 (EO27PO39EO27) are triblock copolymers of ethylene oxide (EO) and propylene oxide (PO), which have the same hydrophobic PO block. We studied aqueous solutions of these two copolymers by the conjoint use of differential scanning calorimetry (DSC), rheology, and small-angle X-ray scattering (SAXS). The results showed that the temperature-induced micellization of aqueous solutions of F88 and P85 was a progressive process followed by gelation for sufficiently concentrated samples. Gelation was due to the ordered packing of micelles under a hexagonal compact (HC) structure for P85 and a body-centered cubic (BCC) phase for F88. Importantly, the phase diagram of F88/P85 mixtures in water was elucidated and sho...
Phase behavior of a PEO-PPO-PEO (Pluronic P103) triblock copolymer in water is investigated using sm...
The solution properties of dilute aqueous solutions of poly(ethylene oxide)-poly(propylene oxide)-po...
The phase behavior of two types of poly(ethylene oxide)/ poly(propylene oxide) (PEO/PPO) copolymers ...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
Aqueous solutions of poly(ethylene oxide-b-( -lactic acid-co-glycolic acid)-b-ethylene oxide) with t...
The phase behavior of poly(ethylene oxide) - poly(propylene oxide) - poly(ethylene oxide), PEO-PPO-P...
The phase behavior of the three-component PEO-PPO-PEO/dextradwater system has been studied. Pluronic...
Poly(ethylene oxide)-poly(propylene oxide)-poly(ethylene oxide) ((EO)(n)-(PO)(m)-(EO)(n)) block copo...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
The phase behavior of two types of poly(ethylene oxide)/ poly(propylene oxide) (PEO/PPO) copolymers ...
Phase behavior of a PEO-PPO-PEO (Pluronic P103) triblock copolymer in water is investigated using sm...
The solution properties of dilute aqueous solutions of poly(ethylene oxide)-poly(propylene oxide)-po...
The phase behavior of two types of poly(ethylene oxide)/ poly(propylene oxide) (PEO/PPO) copolymers ...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
HypothesisThe micellization of block copolymers of poly(ethylene oxide) (PEO) and poly(propylene oxi...
Aqueous solutions of poly(ethylene oxide-b-( -lactic acid-co-glycolic acid)-b-ethylene oxide) with t...
The phase behavior of poly(ethylene oxide) - poly(propylene oxide) - poly(ethylene oxide), PEO-PPO-P...
The phase behavior of the three-component PEO-PPO-PEO/dextradwater system has been studied. Pluronic...
Poly(ethylene oxide)-poly(propylene oxide)-poly(ethylene oxide) ((EO)(n)-(PO)(m)-(EO)(n)) block copo...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
Aqueous solutions of F127 pluronic systems exhibit an interesting thermal gelation above a certain c...
The phase behavior of two types of poly(ethylene oxide)/ poly(propylene oxide) (PEO/PPO) copolymers ...
Phase behavior of a PEO-PPO-PEO (Pluronic P103) triblock copolymer in water is investigated using sm...
The solution properties of dilute aqueous solutions of poly(ethylene oxide)-poly(propylene oxide)-po...
The phase behavior of two types of poly(ethylene oxide)/ poly(propylene oxide) (PEO/PPO) copolymers ...