The potential biomedical application of three new quaternary Zr alloys, namely Zr6Ti15Nb4Al, Zr32Ti15Nb4Al, and Zr49Ti15Nb4Al, was evaluated in vitro using electrochemical methods complemented with surface analysis of corrosion resistance. Cyclic potentiodynamic polarization (CCP) and electrochemical impedance spectroscopy (EIS) tests were performed in Ringer’s solution at 37 ºC. The electrochemical behavior of the ZrTiNbAl quaternary alloys was consistent with the formation of passivating oxide films on the surfaces of these materials. Localized breakdown of the oxide layer occurred on Zr6Ti15Nb4Al and Zr32Ti15Nb4Al alloys subjected to positive anodic polarization, a feature confirmed by scanning electron microscopy (SEM) on retrieved samp...
Titanium alloys show attractive properties for biomedical applications where the most important fact...
Ti-6Al-4V alloy has been widely used in restorative surgery due to its high corrosion resistance and...
This paper addresses on the electrochemical behaviour of three TiMo alloys exposed to simulated phys...
The electrochemical behaviour of three ZrTi alloys (Zr5Ti, Zr25Ti and Zr45Ti) in Ringer’s solution h...
The in vitro corrosion behavior of four Zrâ€based alloys (Zr97.5Nb1.5VM1.0; VM 1â„4 valve metal: T...
The in vitro corrosion behavior and biocompatibility of two Zr alloys, Zr-2.5Nb, employed for the ma...
Binary Zr-Ti alloys spontaneously develop a tenacious and compact oxide layer when their fresh surf...
Oxidation in air of ZrTi alloys at 500 ºC for 2 h produces oxide-covered materials with a very high ...
The degradation characteristics of hydroxyapatite-zirconia-silver films (HA-ZrO2-Ag) coatings on thr...
A new titanium base Ti-21Nb-15Ta-6Zr alloy covered with hydroxyapatite-zirconia (HA-ZrO2) by pulsed ...
In this work, the effects of Nb content on microstructure and corrosion behaviors of biomedical Zr-N...
The present study explores the in vitro and in vivo responses of new multifunctional quaternary bet...
Purpose: We assessed in vitro the corrosion behavior and biocompatibility of four Zr-based alloys (Z...
Corrosion behaviour of the studied Ti20Mo alloy together with the currently used metallic biomateria...
Zirconium is a potential material for permanent implants. In particular, surface modification induce...
Titanium alloys show attractive properties for biomedical applications where the most important fact...
Ti-6Al-4V alloy has been widely used in restorative surgery due to its high corrosion resistance and...
This paper addresses on the electrochemical behaviour of three TiMo alloys exposed to simulated phys...
The electrochemical behaviour of three ZrTi alloys (Zr5Ti, Zr25Ti and Zr45Ti) in Ringer’s solution h...
The in vitro corrosion behavior of four Zrâ€based alloys (Zr97.5Nb1.5VM1.0; VM 1â„4 valve metal: T...
The in vitro corrosion behavior and biocompatibility of two Zr alloys, Zr-2.5Nb, employed for the ma...
Binary Zr-Ti alloys spontaneously develop a tenacious and compact oxide layer when their fresh surf...
Oxidation in air of ZrTi alloys at 500 ºC for 2 h produces oxide-covered materials with a very high ...
The degradation characteristics of hydroxyapatite-zirconia-silver films (HA-ZrO2-Ag) coatings on thr...
A new titanium base Ti-21Nb-15Ta-6Zr alloy covered with hydroxyapatite-zirconia (HA-ZrO2) by pulsed ...
In this work, the effects of Nb content on microstructure and corrosion behaviors of biomedical Zr-N...
The present study explores the in vitro and in vivo responses of new multifunctional quaternary bet...
Purpose: We assessed in vitro the corrosion behavior and biocompatibility of four Zr-based alloys (Z...
Corrosion behaviour of the studied Ti20Mo alloy together with the currently used metallic biomateria...
Zirconium is a potential material for permanent implants. In particular, surface modification induce...
Titanium alloys show attractive properties for biomedical applications where the most important fact...
Ti-6Al-4V alloy has been widely used in restorative surgery due to its high corrosion resistance and...
This paper addresses on the electrochemical behaviour of three TiMo alloys exposed to simulated phys...