Textured n-type Bi₂-xSmxTe₂.₇Se₀.₃ compounds with x ¼ 0; 0.005; 0.02 and 0.05 have been prepared by microwave-solvothermal synthesis of starting powders and spark plasma sintering of bulk materials. Texturing [001] axis coincided with direction of spark plasma sintering pressuring. With increasing x, (i) an average lateral size of grains in the samples is decreasing; (ii) the Lotgering factor characterizing a degree of preferential orientation of the grains is increasing; (iii) anomalies of all the thermoelectric properties, related to onset of intrinsic conductivity, are shifted to higher temperature
Novel cermet Bi₂Te₂.₁Se₀.₉+0.33 wt% Co composite has been prepared via spark plasma sintering (SPS) ...
In the frame of the current research, the p-type Bi2Te3 doped (GeTe)(0.95)(Bi2Te3)(0.05) alloy compo...
Bi2Te3-based alloys are the best thermoelectric materials near room temperature and Bi2(TeSe)3 alloy...
The Bi2Te3, Bi1.9Lu0.1Te3 and Bi1.9Tm0.1Te3 thermoelectrics of n-type conductivity have been prepare...
Solvothermal synthesis and spark plasma sintering were applied to prepare Te-rich Bi₂₋ₓGdₓTe₃₊y comp...
Textured Bi₂₋ₓSmₓTe₂.₇Se₀.₃ compounds with x ¼ 0; 0.005; 0.01; 0.02; 0.05; 0.1; 0.2 and 0.3 were pre...
The Gd-doped Bi₂Te₃ compounds were prepared by solvothermal synthesis and spark plasma sintering. It...
Nanopowders of Bi₂Te₃ and R₀.₁Bi₁.₉Te₃ (where R = Er, Tm, Yb, Lu) are obtained by microwave solvothe...
AbstractNanopowders of elements doped Bi2Te3 thermoelectric alloy R0.2Bi1.8Te3 (R=Ce, Y and Sm) were...
peer reviewedBulk p and n-type bismuth tellurides were prepared using spark plasma texturization met...
The widespread application of thermoelectric (TE) technology demands high-performance materials, whi...
Over the past two decades several nano-structuring methods have helped improve the figure of merit (...
A high thermoelectric figure of merit (ZT) in state-of-the-art bismuth antimony telluride (BST) comp...
Spark plasma sintering (SPS) was applied to prepare textured Bi₁.₉Gd₀.₁Te₃ compounds with various gr...
Zintl compound n-type Mg_3(Sb,Bi)_2 was recently found to exhibit excellent thermoelectric figure of...
Novel cermet Bi₂Te₂.₁Se₀.₉+0.33 wt% Co composite has been prepared via spark plasma sintering (SPS) ...
In the frame of the current research, the p-type Bi2Te3 doped (GeTe)(0.95)(Bi2Te3)(0.05) alloy compo...
Bi2Te3-based alloys are the best thermoelectric materials near room temperature and Bi2(TeSe)3 alloy...
The Bi2Te3, Bi1.9Lu0.1Te3 and Bi1.9Tm0.1Te3 thermoelectrics of n-type conductivity have been prepare...
Solvothermal synthesis and spark plasma sintering were applied to prepare Te-rich Bi₂₋ₓGdₓTe₃₊y comp...
Textured Bi₂₋ₓSmₓTe₂.₇Se₀.₃ compounds with x ¼ 0; 0.005; 0.01; 0.02; 0.05; 0.1; 0.2 and 0.3 were pre...
The Gd-doped Bi₂Te₃ compounds were prepared by solvothermal synthesis and spark plasma sintering. It...
Nanopowders of Bi₂Te₃ and R₀.₁Bi₁.₉Te₃ (where R = Er, Tm, Yb, Lu) are obtained by microwave solvothe...
AbstractNanopowders of elements doped Bi2Te3 thermoelectric alloy R0.2Bi1.8Te3 (R=Ce, Y and Sm) were...
peer reviewedBulk p and n-type bismuth tellurides were prepared using spark plasma texturization met...
The widespread application of thermoelectric (TE) technology demands high-performance materials, whi...
Over the past two decades several nano-structuring methods have helped improve the figure of merit (...
A high thermoelectric figure of merit (ZT) in state-of-the-art bismuth antimony telluride (BST) comp...
Spark plasma sintering (SPS) was applied to prepare textured Bi₁.₉Gd₀.₁Te₃ compounds with various gr...
Zintl compound n-type Mg_3(Sb,Bi)_2 was recently found to exhibit excellent thermoelectric figure of...
Novel cermet Bi₂Te₂.₁Se₀.₉+0.33 wt% Co composite has been prepared via spark plasma sintering (SPS) ...
In the frame of the current research, the p-type Bi2Te3 doped (GeTe)(0.95)(Bi2Te3)(0.05) alloy compo...
Bi2Te3-based alloys are the best thermoelectric materials near room temperature and Bi2(TeSe)3 alloy...