*Akgün, Mahir ( Aksaray, Yazar )This study focuses on optimization of cutting conditions and numerical analysis of flank wear in milling of Inconel 625 superalloy using PVD AlTiN and CVD TiCN/Al2O3/TiN-coated carbide inserts. The milling experiments have been performed in CNC vertical machining centre according to Taguchi L18 orthogonal array. Finite element modelling of tool wear was performed using Deform 3D software. Analysis of variance was utilized to define the influences of the milling conditions on Vb. The results showed that the feed rate (with 41.5% contribution rate) is the most important parameter affecting Vb. The linear and quadratic regression analyses were used to estimate the results of the test. The regression analysis res...
AbstractThe demand for the use of nickel-based superalloy such as Inconel 718 is increasing in aeros...
Cobalt base superalloys are used extensively in applications requiring good wear, corrosion and heat...
This paper focuses on an analysis of tool wear and optimum machining parameter in the induction assi...
*Akgün, Mahir ( Aksaray, Yazar )The main objective of this work is to experimentally investigate and...
Original scientific paper In this study, the effects of cutting speed, milling direction (down milli...
A comprehensive study and FEM simulation of ball nose end milling on tool wear behavior and chip for...
This paper discuss of the Optimization of Tool Life in Milling. The objective of the paper is to obt...
Applying cutting tool with longer functioning time is a vital issue in machining of the nickel-based...
Applying cutting tool with longer functioning time is a vital issue in machining of the nickel-based...
Inconel 718 is a difficult-to-cut nickel-based superalloy commonly used in aerospace industry. This ...
Highly automated CNC end milling machines in manufacturing industry requires reliable model for pred...
AbstractThis work presents a statistical approach for optimization of dry turning parameters of Inco...
385-393Inconel 600 is a nickel-based super alloy with applications in the field of Aerospace, Nuclea...
Cutting tools nearly make up 30% of all the manufacturing cost. Modeling and simulation of machining...
The study aims at optimization of cutting parameters in CNC End milling of Aluminum Alloy 6082. CNC ...
AbstractThe demand for the use of nickel-based superalloy such as Inconel 718 is increasing in aeros...
Cobalt base superalloys are used extensively in applications requiring good wear, corrosion and heat...
This paper focuses on an analysis of tool wear and optimum machining parameter in the induction assi...
*Akgün, Mahir ( Aksaray, Yazar )The main objective of this work is to experimentally investigate and...
Original scientific paper In this study, the effects of cutting speed, milling direction (down milli...
A comprehensive study and FEM simulation of ball nose end milling on tool wear behavior and chip for...
This paper discuss of the Optimization of Tool Life in Milling. The objective of the paper is to obt...
Applying cutting tool with longer functioning time is a vital issue in machining of the nickel-based...
Applying cutting tool with longer functioning time is a vital issue in machining of the nickel-based...
Inconel 718 is a difficult-to-cut nickel-based superalloy commonly used in aerospace industry. This ...
Highly automated CNC end milling machines in manufacturing industry requires reliable model for pred...
AbstractThis work presents a statistical approach for optimization of dry turning parameters of Inco...
385-393Inconel 600 is a nickel-based super alloy with applications in the field of Aerospace, Nuclea...
Cutting tools nearly make up 30% of all the manufacturing cost. Modeling and simulation of machining...
The study aims at optimization of cutting parameters in CNC End milling of Aluminum Alloy 6082. CNC ...
AbstractThe demand for the use of nickel-based superalloy such as Inconel 718 is increasing in aeros...
Cobalt base superalloys are used extensively in applications requiring good wear, corrosion and heat...
This paper focuses on an analysis of tool wear and optimum machining parameter in the induction assi...