To apply the duplex type low-carbon medium-manganese steel to the hot/warm-forging and -stamping products, the influence of cooling process routes immediately after intercritical annealing such as air-cooling (AC) and isothermal transformation (IT) processes on the impact toughness of 0.2%C-1.5%Si-5%Mn (in mass %) duplex type medium-Mn (D-MMn) steel was investigated. Moreover the microstructural and tensile properties were also investigated. The AC process increased the volume fraction of reverted austenite but decreased the thermal and mechanical stability in the D-MMn steel, compared to the IT process. The AC process increased the tensile strength but decreased the total elongation. The Charpy V-notch impact value and ductile-brittle tran...
The current work aims at obtaining optimum amount of austenite after processing of a medium manganes...
The microstructural evolution with varying intercritical-annealing temperatures of medium-Mn (alpha ...
International audienceThe mechanical behaviour and fracture were studied in a Fe-5Mn-2.5Al-0.2C (in ...
In this study, a novel multi-step heat treatment method, including intercritical annealing and tempe...
An investigation has been made into the influence of intercritical annealing on the tensile and impa...
Intercritical annealing (IA) heat treatments are implemented to a variety of steels with the general...
The mechanical properties after tempering and intercritical annealing of medium manganese steels wit...
A medium Mn steel has been designed to achieve an excellent combination of strength and ductility b...
The present work reports the effect of different initial microstructures on reverse transformation k...
Medium manganese steels which belong to the 3rd generation advanced high strength steels are a promi...
Medium-Mn steels are characterized by ultrafine-grained (UFG) duplex microstructure consisting of fe...
DoctorThe present work reports the effect of different initial microstructures on intercritical anne...
The microstructure and mechanical properties of intercritically annealed medium Mn steel are depende...
This paper reports the theoretical design of time-temperature matrix for intercritical annealing of ...
New medium Mn steels for forged components, in combination with a new heat treatment, are presented....
The current work aims at obtaining optimum amount of austenite after processing of a medium manganes...
The microstructural evolution with varying intercritical-annealing temperatures of medium-Mn (alpha ...
International audienceThe mechanical behaviour and fracture were studied in a Fe-5Mn-2.5Al-0.2C (in ...
In this study, a novel multi-step heat treatment method, including intercritical annealing and tempe...
An investigation has been made into the influence of intercritical annealing on the tensile and impa...
Intercritical annealing (IA) heat treatments are implemented to a variety of steels with the general...
The mechanical properties after tempering and intercritical annealing of medium manganese steels wit...
A medium Mn steel has been designed to achieve an excellent combination of strength and ductility b...
The present work reports the effect of different initial microstructures on reverse transformation k...
Medium manganese steels which belong to the 3rd generation advanced high strength steels are a promi...
Medium-Mn steels are characterized by ultrafine-grained (UFG) duplex microstructure consisting of fe...
DoctorThe present work reports the effect of different initial microstructures on intercritical anne...
The microstructure and mechanical properties of intercritically annealed medium Mn steel are depende...
This paper reports the theoretical design of time-temperature matrix for intercritical annealing of ...
New medium Mn steels for forged components, in combination with a new heat treatment, are presented....
The current work aims at obtaining optimum amount of austenite after processing of a medium manganes...
The microstructural evolution with varying intercritical-annealing temperatures of medium-Mn (alpha ...
International audienceThe mechanical behaviour and fracture were studied in a Fe-5Mn-2.5Al-0.2C (in ...