In-situ analysis of the surface of a working selective oxidation catalyst is an essential yet rarely conducted experiment in attempts to derive structure-function relationships. The case study of n-butane oxidation over vanadyl pyrophosphate (VPP) is used to develop a general working hypothesis and to illustrate that the molecular properties of the substrate set boundary conditions on the surface chemical properties of the catalyst. Experiments using in-situ X-ray photoelectron spectroscopy (XPS) and in-situ low energy X-ray absorption spectroscopy are used to derive compositional, electronic, and geometric structural information of the surface of the working VPP. These data allow the conclusion that a surface phase different from VPP must ...
V P O catalysts supported on the surface of silica and titania particles were studied and compared w...
In order to close the pressure gap in the investigation of catalyst surfaces under real operation co...
The effect of Nb when used as a promoter for vanadyl pyrophosphate, the catalyst for the oxidation o...
In-situ analysis of the surface of a working selective oxidation catalyst is an essential yet rarely...
In-situ analysis of the surface of a working selective oxidation catalyst is an essential yet rarely...
In situ X-ray absorption spectroscopy (XAS) and in situ X-ray photoelectron spectroscopy (XPS) have ...
In situ X-ray absorption spectroscopy (XAS) and in situ X-ray photoelectron spectroscopy (XPS) have ...
oraleIn the present work we report on the transient reactivity and the changes of the surface oxidat...
oraleIn the present work we report on the transient reactivity and the changes of the surface oxidat...
The surface acidity of two (VO)2P2O7 catalysts with similar specific activities per square meter of ...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
V P O catalysts supported on the surface of silica and titania particles were studied and compared w...
In order to close the pressure gap in the investigation of catalyst surfaces under real operation co...
V P O catalysts supported on the surface of silica and titania particles were studied and compared w...
In order to close the pressure gap in the investigation of catalyst surfaces under real operation co...
The effect of Nb when used as a promoter for vanadyl pyrophosphate, the catalyst for the oxidation o...
In-situ analysis of the surface of a working selective oxidation catalyst is an essential yet rarely...
In-situ analysis of the surface of a working selective oxidation catalyst is an essential yet rarely...
In situ X-ray absorption spectroscopy (XAS) and in situ X-ray photoelectron spectroscopy (XPS) have ...
In situ X-ray absorption spectroscopy (XAS) and in situ X-ray photoelectron spectroscopy (XPS) have ...
oraleIn the present work we report on the transient reactivity and the changes of the surface oxidat...
oraleIn the present work we report on the transient reactivity and the changes of the surface oxidat...
The surface acidity of two (VO)2P2O7 catalysts with similar specific activities per square meter of ...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
The surface of an activated vanadium phosphorus oxide (VPO) catalyst was investigated by means of in...
V P O catalysts supported on the surface of silica and titania particles were studied and compared w...
In order to close the pressure gap in the investigation of catalyst surfaces under real operation co...
V P O catalysts supported on the surface of silica and titania particles were studied and compared w...
In order to close the pressure gap in the investigation of catalyst surfaces under real operation co...
The effect of Nb when used as a promoter for vanadyl pyrophosphate, the catalyst for the oxidation o...