Nonequilibrium collective phenomena and effects of nonlinear pattern formation play the crucial role in the onset of pitting corrosion on stainless steels. Such materials are naturally protected by the oxide layer covering their surface. The onset of pitting corrosion involves the development of microscopic metastable pits, each persisting for about a second. As proposed in our publications and confirmed in subsequent experiments, sudden transition to active corrosion results from chain reproduction of metastable pits on the stainless steel surface leading to an autocatalytic explosion
The bi-modal characteristic of general or 'uniform' corrosion, or corrosion as measured by mass loss...
The Cl--induced corrosion of metals and alloys is of relevance to a wide range of engineered materia...
C04-Passivity and Localized CorrosionInternational audiencePrediction of material lifetime such as s...
Nonequilibrium collective phenomena and effects of nonlinear pattern formation play the crucial role...
Stainless steels undergo a sharp rise in pitting corrosion rate as the potential, solution concentra...
Stochastic temporal and spatiotemporal models of metastable pitting on a metal surface are presented...
A spatiotemporal model of metastable pitting at a homogeneous metal surface under potentiostatic con...
A critical transition potential is shown to be associated with the abrupt increase in the number of ...
Mechanistic aspects of the initiation and early stages of growth of pitting corrosion on stainless s...
Two types of experiments on metastable pitting are carried out in NaCl solutions, one with galvanica...
It is often believed that pitting events are stochastic without any spatial or temporal effect on ea...
A previously developed spatiotemporal model of the interactions among metastable pits on homogeneous...
A stochastic model for localized corrosion is investigated both analytically and numerically. A feat...
For any particular stainless steel, a critical pitting temperature (CPT) can be measured, below whic...
In situ observations of pitting corrosion as it spreads across the surface of stainless steel were c...
The bi-modal characteristic of general or 'uniform' corrosion, or corrosion as measured by mass loss...
The Cl--induced corrosion of metals and alloys is of relevance to a wide range of engineered materia...
C04-Passivity and Localized CorrosionInternational audiencePrediction of material lifetime such as s...
Nonequilibrium collective phenomena and effects of nonlinear pattern formation play the crucial role...
Stainless steels undergo a sharp rise in pitting corrosion rate as the potential, solution concentra...
Stochastic temporal and spatiotemporal models of metastable pitting on a metal surface are presented...
A spatiotemporal model of metastable pitting at a homogeneous metal surface under potentiostatic con...
A critical transition potential is shown to be associated with the abrupt increase in the number of ...
Mechanistic aspects of the initiation and early stages of growth of pitting corrosion on stainless s...
Two types of experiments on metastable pitting are carried out in NaCl solutions, one with galvanica...
It is often believed that pitting events are stochastic without any spatial or temporal effect on ea...
A previously developed spatiotemporal model of the interactions among metastable pits on homogeneous...
A stochastic model for localized corrosion is investigated both analytically and numerically. A feat...
For any particular stainless steel, a critical pitting temperature (CPT) can be measured, below whic...
In situ observations of pitting corrosion as it spreads across the surface of stainless steel were c...
The bi-modal characteristic of general or 'uniform' corrosion, or corrosion as measured by mass loss...
The Cl--induced corrosion of metals and alloys is of relevance to a wide range of engineered materia...
C04-Passivity and Localized CorrosionInternational audiencePrediction of material lifetime such as s...