In this study, the influence of the processing conditions and the addition of trans-polyoctenylene rubber (TOR) on Mooney viscosity, tensile properties, hardness, tearing resistance, and resilience of natural rubber/styrene-butadiene rubber blends was investigated. The results obtained are explained in light of dynamic mechanical and morphological analyses. Increasing processing time produced a finer blend morphology, which resulted in an improvement in the mechanical properties. The addition of TOR involved an increase in hardness, a decrease in tear resistance, and no effect on the resilience. It resulted in a large decrease in the Mooney viscosity and a slight decrease in the tensile properties if the components of the compounds were not...
Natural rubber remains today an unavoidable elastomer for the manufacture of technical articles such...
The use of methyl methacrylate butadiene styrene (MBS) as a compatibilizer for natural rubber (NR) a...
Tensile and fracture properties of PA6,6/PP blends with 20wt% styrene-ethylene/butylene-styrene trib...
Blendas poliméricas são largamente utilizadas nas indústrias de pneus por causa de seu baixo custo e...
The rubber blends for rubber roller were prepared with natural rubber, styrene-butadiene rubber and ...
ABSTRACT: With a view to improve degradation properties of natural rubber on prolonged cure at moder...
In this study, the influence of Trans- Polyoctylene Rubber (TOR) as a compatibilizer on the cure cha...
The mechanical properties, natural rubber (NR) blends were studied in various ratio; 100:0, 85:15, 7...
Thermoplastic natural rubber (TPNR) those produced by blending of thermoplastics and natural rubber...
In this work, the effect of mixing temperature (Tmix) on the mechanical, rheological, and morphologi...
Synthetic rubber on the other hand is a rubber which is synthesized chemically. Styrene-butadiene ru...
Blending of polymers can create new materials with a broad spectrum of physicochemical properties an...
Fabrication of partially biobased poly(trimethylene terephthalate) (PTT) elastomeric blends was don...
Pyrolytic carbon black (CBp) and pyrolytic oil (Op) made from used tires were used in natural rubber...
Blends of aliphatic polyketone terpolymer and a core-shell rubber (CSR) were melt processed with var...
Natural rubber remains today an unavoidable elastomer for the manufacture of technical articles such...
The use of methyl methacrylate butadiene styrene (MBS) as a compatibilizer for natural rubber (NR) a...
Tensile and fracture properties of PA6,6/PP blends with 20wt% styrene-ethylene/butylene-styrene trib...
Blendas poliméricas são largamente utilizadas nas indústrias de pneus por causa de seu baixo custo e...
The rubber blends for rubber roller were prepared with natural rubber, styrene-butadiene rubber and ...
ABSTRACT: With a view to improve degradation properties of natural rubber on prolonged cure at moder...
In this study, the influence of Trans- Polyoctylene Rubber (TOR) as a compatibilizer on the cure cha...
The mechanical properties, natural rubber (NR) blends were studied in various ratio; 100:0, 85:15, 7...
Thermoplastic natural rubber (TPNR) those produced by blending of thermoplastics and natural rubber...
In this work, the effect of mixing temperature (Tmix) on the mechanical, rheological, and morphologi...
Synthetic rubber on the other hand is a rubber which is synthesized chemically. Styrene-butadiene ru...
Blending of polymers can create new materials with a broad spectrum of physicochemical properties an...
Fabrication of partially biobased poly(trimethylene terephthalate) (PTT) elastomeric blends was don...
Pyrolytic carbon black (CBp) and pyrolytic oil (Op) made from used tires were used in natural rubber...
Blends of aliphatic polyketone terpolymer and a core-shell rubber (CSR) were melt processed with var...
Natural rubber remains today an unavoidable elastomer for the manufacture of technical articles such...
The use of methyl methacrylate butadiene styrene (MBS) as a compatibilizer for natural rubber (NR) a...
Tensile and fracture properties of PA6,6/PP blends with 20wt% styrene-ethylene/butylene-styrene trib...