The origin and scaling of the current measured during steady electrospinning of polymer solutions in organic solvents are considered. For a specified electric field strength E, flow rate Q, and conductivity K, the total measured current is shown empirically to scale as Itotal ∼ EQ0.5K0.4, for a wide variety of polymer solutions with different electrical conductivities. It is also shown that Itotal is composed of two distinct components: one that varies linearly with E, and another that is independent of E, but varies with the conductivity K of the fluid and the flow rate Q. The experimental evidence suggests that the latter component arises due to a secondary electrospray emanating from the surface of the jet. The consequence of this second...
Abstract: We performed an extensive characterization of an electrospinning process to evaluate how t...
The emerging technology of manufacturing of polymer nanofibers by the electrospinning method is addr...
Several polyurethane solutions of the same composition but varying temperature (25, 50, 75 and 100 °...
The electric currents between electrodes in the electrospinning process are based on the movement of...
This paper suggests an approximate formula predicting the electric current in the electrospinning...
Electrospinning has become a widely implemented technique for the generation of nonwoven mats that a...
Electrospinning is a method of using high voltage electric fields to transform polymer solutions int...
Electrospinning produces submicron fibers from a wide range of polymer/solvent systems that enable a...
With the rapid development of electrospinning, how to control the spinning drawing process is becomi...
Needleless electrospinning is the process of forming thin material fibers from the open surface of i...
Producing nanofiber-diameter polymeric fibers presents an attractive and robust approach toward the ...
The electrospinning process uses electrical force to produce nanofibers. A charged droplet acquires ...
Thesis (M.Sc.Eng.) PLEASE NOTE: Boston University Libraries did not receive an Authorization To Mana...
Solvent-polymer interactions critically influence not only the viscoelasticity and the critical mini...
The most important characteristics of the electrospun fibers are their internal morphology and their...
Abstract: We performed an extensive characterization of an electrospinning process to evaluate how t...
The emerging technology of manufacturing of polymer nanofibers by the electrospinning method is addr...
Several polyurethane solutions of the same composition but varying temperature (25, 50, 75 and 100 °...
The electric currents between electrodes in the electrospinning process are based on the movement of...
This paper suggests an approximate formula predicting the electric current in the electrospinning...
Electrospinning has become a widely implemented technique for the generation of nonwoven mats that a...
Electrospinning is a method of using high voltage electric fields to transform polymer solutions int...
Electrospinning produces submicron fibers from a wide range of polymer/solvent systems that enable a...
With the rapid development of electrospinning, how to control the spinning drawing process is becomi...
Needleless electrospinning is the process of forming thin material fibers from the open surface of i...
Producing nanofiber-diameter polymeric fibers presents an attractive and robust approach toward the ...
The electrospinning process uses electrical force to produce nanofibers. A charged droplet acquires ...
Thesis (M.Sc.Eng.) PLEASE NOTE: Boston University Libraries did not receive an Authorization To Mana...
Solvent-polymer interactions critically influence not only the viscoelasticity and the critical mini...
The most important characteristics of the electrospun fibers are their internal morphology and their...
Abstract: We performed an extensive characterization of an electrospinning process to evaluate how t...
The emerging technology of manufacturing of polymer nanofibers by the electrospinning method is addr...
Several polyurethane solutions of the same composition but varying temperature (25, 50, 75 and 100 °...