Thesis (Ph.D.)--Massachusetts Institute of Technology, Dept. of Materials Science and Engineering, 1982.MICROFICHE COPY AVAILABLE IN ARCHIVES AND SCIENCEIncludes bibliographical references.by Charles Hubert Smith.Ph.D
Thesis Abstract: Laser powder bed fusion (LPBF), a specialization within additive manufacturing, is ...
Alloy strengthening mechanisms - strengthening by fine particle dispersion, and structure and proper...
Nickel-based superalloys have the ability to form protective surface oxide scales at high temperatur...
An experimental oxide dispersion strengthened (ODS) alloy based on the B-1900 composition was produc...
There were three nickel-base alloys containing up to 18 wt. % of refractory metal examined initially...
Stable dispersion hardened materials produced by controlled cleaning and pressing of ball milled ble...
The sintered aluminum powder (SAP) technique of dispersion strengthening (formation of an oxide disp...
292 p.Thesis (Ph.D.)--University of Illinois at Urbana-Champaign, 1987.A study of reduced chromium c...
Oxide-Dispersion-Strengthened (ODS) Nickel-Based superalloy has been drawn a huge attention and deve...
An experimental oxide dispersion strengthened (ODS) alloy, WAZ-D, derived from the WAZ-20 compositio...
The Ni-base superalloys are a popular range of materials for study following consolidation by additi...
Superalloy represents a class of high temperature / high performance material, which became avail...
Nickel-base superalloys obtain high temperature mechanical properties through formation of precipita...
An investigation was conducted to determine whether a nickel - 2-volume-percent alumina dispersion-s...
Thesis Abstract: Laser powder bed fusion (LPBF), a specialization within additive manufacturing, is ...
Thesis Abstract: Laser powder bed fusion (LPBF), a specialization within additive manufacturing, is ...
Alloy strengthening mechanisms - strengthening by fine particle dispersion, and structure and proper...
Nickel-based superalloys have the ability to form protective surface oxide scales at high temperatur...
An experimental oxide dispersion strengthened (ODS) alloy based on the B-1900 composition was produc...
There were three nickel-base alloys containing up to 18 wt. % of refractory metal examined initially...
Stable dispersion hardened materials produced by controlled cleaning and pressing of ball milled ble...
The sintered aluminum powder (SAP) technique of dispersion strengthening (formation of an oxide disp...
292 p.Thesis (Ph.D.)--University of Illinois at Urbana-Champaign, 1987.A study of reduced chromium c...
Oxide-Dispersion-Strengthened (ODS) Nickel-Based superalloy has been drawn a huge attention and deve...
An experimental oxide dispersion strengthened (ODS) alloy, WAZ-D, derived from the WAZ-20 compositio...
The Ni-base superalloys are a popular range of materials for study following consolidation by additi...
Superalloy represents a class of high temperature / high performance material, which became avail...
Nickel-base superalloys obtain high temperature mechanical properties through formation of precipita...
An investigation was conducted to determine whether a nickel - 2-volume-percent alumina dispersion-s...
Thesis Abstract: Laser powder bed fusion (LPBF), a specialization within additive manufacturing, is ...
Thesis Abstract: Laser powder bed fusion (LPBF), a specialization within additive manufacturing, is ...
Alloy strengthening mechanisms - strengthening by fine particle dispersion, and structure and proper...
Nickel-based superalloys have the ability to form protective surface oxide scales at high temperatur...