Effect of intermediate thermomechanical treatment on tensile properties at short-transverse direction, intergranular corrosion, macrostructure and microstructure of 2A97 Al-Li alloy thin plate were studied by tensile testing,intergranular corrosion, EBSD and TEM.The results show that with the increase of compression deformation, the strength and elongation of the alloy increase first and then decrease slightly. When compression deformation is 20%, the grain size of recrystallization is fine and the uniformly dispersed δ' can be found in the grains,δ' phase located in the grain boundary is discontinuously distributed,the tensile property is the best,and the elongation rate is obviously improved;when the compression deformation is 25%, the in...
The main objective of the present investigation is to clarify the origin of the short transverse del...
The isothermal compression tests of 2195 Al-Li alloy annealed at 400 - 490 ℃ and strain rate 0.01-10...
In this study, the effects of hot-rolled processes at different temperatures (420 °C, 450 °C, and 48...
The effect of pre-sretching processing before artificial aging on the microstructures and properties...
AbstractThe intergranular corrosion and exfoliation corrosion of 2195 Al-Li alloy treated by multi-s...
To explore the effective way of grain refinement for 2219 aluminum alloy, the approach of ‘the...
In this study, the microstructural evolution and mechanical properties of Al-Li 2198-T8 (artificiall...
The effect of thermochanical processing on microstructure and mechanical properties of Al-Li-Cu-Zr a...
The mechanical properties and microstructure evolution of the spray formed 2195 alloy extruded sheet...
All industrial unrecrystallized Al-Li-X alloys exhibit a strong tendency to intergranular failure le...
Solution and aging heat treatment are effective means to improve the mechanical properties of Al-Li ...
A 2297 aluminum-lithium alloy was subjected to multi-axial compression (MAC) at 160 °C to obtain dif...
In order to achieve the combination of mechanical and corrosion properties for the Al-Mg-Mn alloy, a...
Two strength-age hardening aluminum-lithium alloys: Al-2.3wt%Li and Al-2.2wt%Li-0.1wt%Zr in two diff...
The mechanical properties of Al-Li solid solution were studied in tensile deformation tests at extre...
The main objective of the present investigation is to clarify the origin of the short transverse del...
The isothermal compression tests of 2195 Al-Li alloy annealed at 400 - 490 ℃ and strain rate 0.01-10...
In this study, the effects of hot-rolled processes at different temperatures (420 °C, 450 °C, and 48...
The effect of pre-sretching processing before artificial aging on the microstructures and properties...
AbstractThe intergranular corrosion and exfoliation corrosion of 2195 Al-Li alloy treated by multi-s...
To explore the effective way of grain refinement for 2219 aluminum alloy, the approach of ‘the...
In this study, the microstructural evolution and mechanical properties of Al-Li 2198-T8 (artificiall...
The effect of thermochanical processing on microstructure and mechanical properties of Al-Li-Cu-Zr a...
The mechanical properties and microstructure evolution of the spray formed 2195 alloy extruded sheet...
All industrial unrecrystallized Al-Li-X alloys exhibit a strong tendency to intergranular failure le...
Solution and aging heat treatment are effective means to improve the mechanical properties of Al-Li ...
A 2297 aluminum-lithium alloy was subjected to multi-axial compression (MAC) at 160 °C to obtain dif...
In order to achieve the combination of mechanical and corrosion properties for the Al-Mg-Mn alloy, a...
Two strength-age hardening aluminum-lithium alloys: Al-2.3wt%Li and Al-2.2wt%Li-0.1wt%Zr in two diff...
The mechanical properties of Al-Li solid solution were studied in tensile deformation tests at extre...
The main objective of the present investigation is to clarify the origin of the short transverse del...
The isothermal compression tests of 2195 Al-Li alloy annealed at 400 - 490 ℃ and strain rate 0.01-10...
In this study, the effects of hot-rolled processes at different temperatures (420 °C, 450 °C, and 48...