One of the key challenges for the development of high-performance fusion materials is to design materials capable of maintaining mechanical and structural integrity under the extreme levels of displacement damage, high temperature and transmutation rates. High-entropy alloys (HEAs) and other concentrated alloys have attracted attention with regards to their performance under fusion conditions. In recent years, a number of investigations of the irradiation responses of HEAs have peaked the community’s interest in them, such as the work of Kumar et al. (2016), who examined Fe27Ni28Mn27Cr18 at doses as high as 10 dpa. In this work, we study Fe28Ni28Mn26Cr18 concentrated multicomponent alloy with irradiation doses as high as 20 dpa. We find the...
ABSTRACT: A CuCrFeTiV high entropy alloy was prepared and irradiated with swift heavy ions in order ...
Ion irradiation is often used to simulate the effects of neutron irradiation due to reduced activati...
As an increasing demand of advanced nuclear fission reactors and fusion facilities, the key requirem...
One of the key challenges for the development of high-performance fusion materials is to design mate...
Four high entropy alloys (HEA), CoCrCuFeNi, Co1.5CrFeNi1.5Ti0.5Mo0.1, both adopting an FCC structure...
Recent developments in the field of materials for future nuclear fusion reactors have led to the des...
As part of the solutions towards resolving the challenges in energy shortage and climate changes, ad...
Understanding the mechanisms of plasticity in structural steels is essential for the operation of ne...
The development of future energy production concepts, such as Gen-IV fission reactors, has increased...
Multiprincipally designed concentrated solid solution alloys, such as high entropy alloys (HEA) and ...
Understanding the mechanical behavior of nanostructured and amorphous materials under harsh environm...
Ferritic/martensitic steels will be used as structural components in next generation nuclear reactor...
Understanding the mechanisms of plasticity in structural steels is essential for the operation of ne...
The irradiation damage behavior is surveyed in the nano-grained GH3535 condition irradiated by He io...
The irradiation effects of high dpa and the ramification on the engineering assessment of reactor co...
ABSTRACT: A CuCrFeTiV high entropy alloy was prepared and irradiated with swift heavy ions in order ...
Ion irradiation is often used to simulate the effects of neutron irradiation due to reduced activati...
As an increasing demand of advanced nuclear fission reactors and fusion facilities, the key requirem...
One of the key challenges for the development of high-performance fusion materials is to design mate...
Four high entropy alloys (HEA), CoCrCuFeNi, Co1.5CrFeNi1.5Ti0.5Mo0.1, both adopting an FCC structure...
Recent developments in the field of materials for future nuclear fusion reactors have led to the des...
As part of the solutions towards resolving the challenges in energy shortage and climate changes, ad...
Understanding the mechanisms of plasticity in structural steels is essential for the operation of ne...
The development of future energy production concepts, such as Gen-IV fission reactors, has increased...
Multiprincipally designed concentrated solid solution alloys, such as high entropy alloys (HEA) and ...
Understanding the mechanical behavior of nanostructured and amorphous materials under harsh environm...
Ferritic/martensitic steels will be used as structural components in next generation nuclear reactor...
Understanding the mechanisms of plasticity in structural steels is essential for the operation of ne...
The irradiation damage behavior is surveyed in the nano-grained GH3535 condition irradiated by He io...
The irradiation effects of high dpa and the ramification on the engineering assessment of reactor co...
ABSTRACT: A CuCrFeTiV high entropy alloy was prepared and irradiated with swift heavy ions in order ...
Ion irradiation is often used to simulate the effects of neutron irradiation due to reduced activati...
As an increasing demand of advanced nuclear fission reactors and fusion facilities, the key requirem...