7 pags. 8 figs.The forced assembly of two immiscible polymers, produced by layer-multiplying co-extrusion, is analyzed by means of USAXS. Comparison of scattering and AFM results sheds light on many details of the nanolayered structure in PET/PC films. The role played by the volume concentration and cold crystallization of PET on the experimental scattering is discussed. The appearance of at least two scattering maxima in all cases, corresponding to higher orders of the same repeating distance, accounts for the high regularity of the developed nanostructure. It is finally shown that long spacing values, derived from a localized area in AFM, are in a good agreement with the USAXS values averaged over much larger areas. © 2008 WILEY-VCM Verla...
International audienceNanochannels and nanowires with diameters ranging from 30 to 400 nm were produ...
We show that the accessible range of length scales of structures deduced with ultra small-angle scat...
The surface morphology and crystallinity of biaxially drawn (BD) and amorphous poly(ethylene terepht...
9 pags. 12 figs.The crystallization behaviour of semicrystalline polymers in structurally confined e...
The orientation and nanostructure of poly (ethylene terephthalate) PET lamellae within ultrathin lay...
17 pags., 7 figs.The present work is concerned with the study of the development of the crystalline ...
Microlayering is an attractive approach for creating designed polymer architectures for specific pur...
7 pags., 9 figs.The absolute intensity of the small-angle X-ray scattering (SAXS) of poly(ethylene t...
We have constructed the Bonse-Hart type Ultra-small-angle X-ray Scattering (USAXS) instrument to stu...
The hidden structural properties of semicrystalline polymer films are revealed by nanofocused X-ray ...
Tailoring the polymer–metal interface is crucial for advanced material design. Vacuum deposition met...
Polymer nanocomposites are usually studied by means of different techniques, being wide angle X - ra...
In this study the microscopic deformation behaviour of amorphous PET during uniaxial tensile tests a...
Experiments have been conducted at the European Synchrotron Radiation Facility (ESRF) at Grenoble (F...
The cold crystallization kinetics of ultra-thin polymeric films (thickness: 10 nm divided by 0...
International audienceNanochannels and nanowires with diameters ranging from 30 to 400 nm were produ...
We show that the accessible range of length scales of structures deduced with ultra small-angle scat...
The surface morphology and crystallinity of biaxially drawn (BD) and amorphous poly(ethylene terepht...
9 pags. 12 figs.The crystallization behaviour of semicrystalline polymers in structurally confined e...
The orientation and nanostructure of poly (ethylene terephthalate) PET lamellae within ultrathin lay...
17 pags., 7 figs.The present work is concerned with the study of the development of the crystalline ...
Microlayering is an attractive approach for creating designed polymer architectures for specific pur...
7 pags., 9 figs.The absolute intensity of the small-angle X-ray scattering (SAXS) of poly(ethylene t...
We have constructed the Bonse-Hart type Ultra-small-angle X-ray Scattering (USAXS) instrument to stu...
The hidden structural properties of semicrystalline polymer films are revealed by nanofocused X-ray ...
Tailoring the polymer–metal interface is crucial for advanced material design. Vacuum deposition met...
Polymer nanocomposites are usually studied by means of different techniques, being wide angle X - ra...
In this study the microscopic deformation behaviour of amorphous PET during uniaxial tensile tests a...
Experiments have been conducted at the European Synchrotron Radiation Facility (ESRF) at Grenoble (F...
The cold crystallization kinetics of ultra-thin polymeric films (thickness: 10 nm divided by 0...
International audienceNanochannels and nanowires with diameters ranging from 30 to 400 nm were produ...
We show that the accessible range of length scales of structures deduced with ultra small-angle scat...
The surface morphology and crystallinity of biaxially drawn (BD) and amorphous poly(ethylene terepht...