The influence of the passive layer properties on the pitting corrosion of 316SS was studied in phosphate—borate buffer containing chloride ions by using potential step and potentiodynamic techniques complemented with scanning electron microscopy. The increase of the anodization time in the passive region decreases the nucleation rate and the mean number of corrosion pits formed onthe 316SS surface. Results are explained through changes in the structure and composition of the passive layer during anodization. Two different Cr(III) species can be voltammetrically detected at short anodization times, an outer weakly bound Cr(III) species which is electroaoxidized to soluble CrO42− and an inner Cr(III) species which is electrooxidized to Cr(VI)...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5%...
Open circuit potential measurements and cyclic voltammetry of chromium and 304 stainless steel in de...
International audienceElectrochemical polarization measurements were combined with surface analysis ...
The pitting corrosion of 316 stainless steel (SS) in phosphate-borate buffer (pH 8.00) containing 0....
The thin adherent oxide layer formed on the metal surface keeps the surface of metal protective from...
International audienceTime of Flight Secondary Ion Mass Spectroscopy, X-Ray Photoelectron Spectrosco...
Passivation is the process of temporary or permanent halt in degradation or corrosion rate of a meta...
This thesis was submitted for the degree of Doctor of Philosophy and awarded by Brunel University.Th...
The pitting corrosion of copper in borate buffer containing sodium chloride is studied by using pote...
The electrochemical behaviour of the highly alloyed austenitic stainless steel UNS N08031 (Alloy 31)...
The electrochemical behaviour of AISI 316 austenitic stainless steel (SS) was investigated in deaera...
The resistance of austenitic stainless steel type 304 to pitting corrosion was studied in solutions ...
Electrochemical response causing pitting corrosion of high-strength high carbon steel wire in deaera...
The chloride ion (Cl⁻) is known as an aggressive species in the aqueous solutions that adsorbs to th...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5%...
Open circuit potential measurements and cyclic voltammetry of chromium and 304 stainless steel in de...
International audienceElectrochemical polarization measurements were combined with surface analysis ...
The pitting corrosion of 316 stainless steel (SS) in phosphate-borate buffer (pH 8.00) containing 0....
The thin adherent oxide layer formed on the metal surface keeps the surface of metal protective from...
International audienceTime of Flight Secondary Ion Mass Spectroscopy, X-Ray Photoelectron Spectrosco...
Passivation is the process of temporary or permanent halt in degradation or corrosion rate of a meta...
This thesis was submitted for the degree of Doctor of Philosophy and awarded by Brunel University.Th...
The pitting corrosion of copper in borate buffer containing sodium chloride is studied by using pote...
The electrochemical behaviour of the highly alloyed austenitic stainless steel UNS N08031 (Alloy 31)...
The electrochemical behaviour of AISI 316 austenitic stainless steel (SS) was investigated in deaera...
The resistance of austenitic stainless steel type 304 to pitting corrosion was studied in solutions ...
Electrochemical response causing pitting corrosion of high-strength high carbon steel wire in deaera...
The chloride ion (Cl⁻) is known as an aggressive species in the aqueous solutions that adsorbs to th...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5...
The pitting corrosion behavior of 301, 304 and 316 austenitic stainless steels in 2M H2SO4 at 0–1.5%...
Open circuit potential measurements and cyclic voltammetry of chromium and 304 stainless steel in de...